Becker R, Pufe T, Kulow S, Giessmann N, Neumann W, Mentlein R, Petersen W
Department of Orthopaedic Surgery, Otto-von-Guericke-University, Leipziger Strasse 44, 39120 Magdeburg, Germany.
J Bone Joint Surg Br. 2004 Sep;86(7):1082-7. doi: 10.1302/0301-620x.86b7.14349.
Our aim was to investigate vascular endothelial growth factor (VEGF) expression after lacerations of a meniscus in a rabbit model. Specimens of meniscus were examined using immunohistochemistry, enzyme-linked immunoassay and the reverse transcription polymerase chain reaction after one, two, five or ten weeks. In the periphery of the meniscus 90% of the lacerations had healed after five and ten weeks, but no healing was observed in the avascular area. Expression of VEGF protein and VEGF mRNA was found in the meniscus of both the operated and the contralateral sites but both were absent in control rabbits which had not undergone operation. The highest expression of VEGF was found in the avascular area after one week (p < 0.001). It then lessened at both the vascular and avascular areas, but still remained greater in comparison with the control meniscus (p < 0.05). Despite greater expression of VEGF, angiogenesis failed at the inner portion. These findings demonstrated the poor healing response in the avascular area which may not be caused by an intrinsic cellular insufficiency to stimulate angiogenesis.
我们的目的是在兔模型中研究半月板撕裂后血管内皮生长因子(VEGF)的表达情况。在1周、2周、5周或10周后,使用免疫组织化学、酶联免疫吸附测定和逆转录聚合酶链反应对半月板标本进行检查。在半月板周边,90%的撕裂伤在5周和10周后愈合,但在无血管区域未观察到愈合情况。在手术侧和对侧半月板中均发现了VEGF蛋白和VEGF mRNA的表达,但未手术的对照兔中均未发现。术后1周,无血管区域VEGF表达最高(p<0.001)。随后,在血管和无血管区域其表达均降低,但与对照半月板相比仍较高(p<0.05)。尽管VEGF表达较高,但内部区域的血管生成仍失败。这些发现表明无血管区域的愈合反应较差,这可能不是由于内在细胞刺激血管生成不足所致。