Suppr超能文献

聚羟基脂肪酸酯橡胶共混物:合成、表征及生物降解

PHA-rubber blends: synthesis, characterization and biodegradation.

作者信息

Bhatt Rachana, Shah Dishma, Patel K C, Trivedi Ujjval

机构信息

Department of Biosciences, Sardar Patel University, Vallabh Vidyanagar 388 120, Gujarat, India.

出版信息

Bioresour Technol. 2008 Jul;99(11):4615-20. doi: 10.1016/j.biortech.2007.06.054. Epub 2007 Aug 30.

Abstract

Medium chain length polyhydroxyalkanoates (mcl-PHA) and different rubbers; namely natural rubber, nitrile rubber and butadiene rubber were blended at room temperature using solution blending technique. Blends constituted 5%, 10% and 15% of mcl-PHA in different rubbers. Thermogravimetric analysis of mcl-PHA showed the melting temperature of the polymer around 50 degrees C. Thermal properties of the synthesized blend were studied by Differential Scanning Calorimetry which confirmed effective blending between the polymers. Blending of mcl-PHA with natural rubber led to the synthesis of a different polymer having the melting point of 90 degrees C. Degradation studies of the blends were carried out using a soil isolate, Pseudomonas sp. 202 for 30 days. Extracellular protein concentration as well as OD660 due to the growth of Pseudomonas sp. 202 was studied. The degradation of blended plastic material, as evidenced by % weight loss after degradation and increase in the growth of organism correlated with the amount of mcl-PHA present in the sample. Growth of Pseudomonas sp. 202 resulted in 14.63%, 16.12% and 3.84% weight loss of PHA:rubber blends (natural, nitrile and butadiene rubber). Scanning electron microscopic studies after 30 days of incubation further confirmed biodegradation of the films.

摘要

中链长度聚羟基脂肪酸酯(mcl-PHA)与不同橡胶,即天然橡胶、丁腈橡胶和丁二烯橡胶,在室温下采用溶液共混技术进行共混。共混物中mcl-PHA在不同橡胶中的含量分别为5%、10%和15%。mcl-PHA的热重分析表明该聚合物的熔点约为50℃。通过差示扫描量热法研究了合成共混物的热性能,证实了聚合物之间的有效共混。mcl-PHA与天然橡胶共混导致合成了一种熔点为90℃的不同聚合物。使用土壤分离菌假单胞菌属202对共混物进行了30天的降解研究。研究了由于假单胞菌属202生长导致的细胞外蛋白质浓度以及OD660。降解后样品的重量损失百分比以及生物体生长的增加证明,共混塑料材料的降解与样品中mcl-PHA的含量相关。假单胞菌属202的生长导致PHA:橡胶共混物(天然橡胶、丁腈橡胶和丁二烯橡胶)的重量损失分别为14.63%、16.12%和3.84%。孵育30天后的扫描电子显微镜研究进一步证实了薄膜的生物降解。