Han Linlin, Okamoto Akira, Fukushima Masayoshi, Okiji Takashi
Division of Cariology, Operative Dentistry and Endodontics, Department of Oral Health Science, Niigata University Graduate School of Medical and Dental Sciences, 5274 Gakkocho-dori, 2-bancho, Chuo-ku, Niigata 951-8514, Japan.
Dent Mater J. 2008 May;27(3):455-65. doi: 10.4012/dmj.27.455.
The purpose of this study was to evaluate the morphological changes of the surfaces of flowable resins eroded by orange juice and alcohol drinks. The tested products were Beautifil Flow BF02 and BF10, Clearfil Majesty LV, Filtek Supreme XT Flowable Restorative, Unifil LoFlo Plus and Filtek Supreme. Filler percentages of flowable resins were calculated after the latter were incinerated at 750 degrees C. Specimens were shaped into a disk form with a diameter of 10 mm and a thickness of 1 mm. Morphological changes were evaluated for the following types of flowable resin surfaces: polished surface, surfaces eroded by 100% orange juice, wine and whisky. Filler percentages of the tested flowable resins ranged between 42 and 78%. Surface degradation was observed for the specimens immersed in acidic and alcoholic drinks, and it was thought that the lower the filler percentage, the greater was the surface degradation. Decomposition of the matrix resin and fallout of the fillers were observed in flowable resins that eroded with acidic and alcoholic drinks.
本研究的目的是评估可流动树脂表面被橙汁和酒精饮料侵蚀后的形态变化。测试产品有Beautifil Flow BF02和BF10、Clearfil Majesty LV、Filtek Supreme XT可流动修复材料、Unifil LoFlo Plus和Filtek Supreme。可流动树脂在750摄氏度下焚烧后计算其填料百分比。将试样制成直径为10毫米、厚度为1毫米的圆盘形式。对以下类型的可流动树脂表面的形态变化进行了评估:抛光表面、被100%橙汁、葡萄酒和威士忌侵蚀的表面。测试的可流动树脂的填料百分比在42%至78%之间。观察到浸泡在酸性和酒精饮料中的试样表面有降解现象,并且认为填料百分比越低,表面降解越大。在被酸性和酒精饮料侵蚀的可流动树脂中观察到基体树脂的分解和填料的脱落。