Suppr超能文献

curing 时间对光固化灯和等离子弧光灯固化的托槽粘接系统粘结强度的影响。

Effect of curing time on the bond strength of a bracket-bonding system cured with a light-emitting diode or plasma arc light.

机构信息

Department of Orthodontics, School of Dentistry, Pontifical Catholic University of Rio Grande do Sul, Porto Alegre, Brazil.

出版信息

Eur J Orthod. 2011 Feb;33(1):55-9. doi: 10.1093/ejo/cjq027. Epub 2010 Jun 17.

Abstract

The purpose of this study was to assess the influence of two light units, a light-emitting diode (LED) and a plasma arc light (PAC), on the shear bond strength (SBS) of brackets bonded to enamel. Ninety bovine teeth were divided into six groups, according to the light-curing unit and exposure times used. In the LED (Ortholux; 3M-Unitek) group, the specimens were light cured for 5, 10, and 15 seconds. In the PAC (Apollo 95E; DenMed Technologies) group, the specimens were light cured for 3, 6, and 9 seconds. The brackets were bonded with Transbond XT (3M-Unitek), stored in distilled water at 37 °C for 24 hours and then submitted to SBS testing in a universal testing machine. The adhesive remnant index (ARI) was used to evaluate the amount of adhesive remaining on the teeth. According to analysis of variance and Tukey multiple comparisons test, the highest mean SBS was obtained with the LED at 15 seconds (16.68 MPa), which did not significantly differ from the LED 10 (14.76 MPa) or 5 (13.92 MPa) second groups (P > 0.05). The LED 10 and 5 second groups were not significantly different from the PAC 9 second group (12.66 MPa) or from the PAC 6 second group (9.96 MPa). The lowest mean SBS was obtained with the PAC 3 second group (8.29 MPa), which did not differ significantly from the PAC 6 second group. The method of light curing did not influence the ARI, with score 3 predominant. The LED at 5 seconds and the PAC at 3 seconds provided sufficient mean SBS to resist either orthodontic or masticatory forces.

摘要

本研究旨在评估两种光源——发光二极管(LED)和等离子弧光灯(PAC)对黏结到釉质的托槽的剪切结合强度(SBS)的影响。将 90 颗牛牙按光固化单元和使用的曝光时间分为 6 组。在 LED(Ortholux;3M-Unitek)组中,样本分别用 5、10 和 15 秒进行光固化。在 PAC(Apollo 95E;DenMed Technologies)组中,样本分别用 3、6 和 9 秒进行光固化。用 Transbond XT(3M-Unitek)黏结托槽,在 37°C 的蒸馏水中储存 24 小时,然后在万能试验机上进行 SBS 测试。用黏附残余指数(ARI)评估牙齿上残留的黏附剂的量。根据方差分析和 Tukey 多重比较检验,LED 组中 15 秒的平均 SBS 最高(16.68 MPa),与 LED 10 秒(14.76 MPa)或 5 秒(13.92 MPa)组无显著差异(P>0.05)。LED 10 秒和 5 秒组与 PAC 9 秒组或 PAC 6 秒组(9.96 MPa)无显著差异。PAC 3 秒组的平均 SBS 最低(8.29 MPa),与 PAC 6 秒组无显著差异。光固化方式对 ARI 没有影响,主要是 3 分。LED 5 秒和 PAC 3 秒提供了足够的平均 SBS 来抵抗正畸或咀嚼力。