饮料对牙釉质表面粗糙度和 pH 值影响的体外研究——触针轮廓仪、变焦距三维扫描显微镜和显微 pH 传感器的应用。

Roughness and pH changes of enamel surface induced by soft drinks in vitro-applications of stylus profilometry, focus variation 3D scanning microscopy and micro pH sensor.

机构信息

Department of Restorative Sciences, Tokyo Medical and Dental University, Tokyo 113-8549, Japan.

出版信息

Dent Mater J. 2011;30(3):404-10. doi: 10.4012/dmj.2010-204. Epub 2011 May 20.

Abstract

This study aimed to evaluate enamel surface roughness (Ra) and pH before and after erosion by soft drinks. Enamel was exposed to a soft drink (cola, orange juice or green tea) for 1, 5 or 60 min; Ra was measured using contact-stylus surface profilometry (SSP) and non-contact focus variation 3D microscope (FVM). Surface pH was measured using a micro pH sensor. Data were analyzed at significance level of alpha=0.05. There was a significant correlation in Ra between SSP and FVM. FVM images showed no changes in the surface morphology after various periods of exposure to green tea. Unlike cola and orange juice, exposure to green tea did not significantly affect Ra or pH. A significant correlation was observed between surface pH and Ra change after exposure to the drinks. Optical surface analysis and micro pH sensor may be useful tools for non-damaging, quantitative assessment of soft drinks erosion on enamel.

摘要

本研究旨在评估软饮料侵蚀前后牙釉质表面粗糙度(Ra)和 pH 值。将牙釉质暴露于软饮料(可乐、橙汁或绿茶)中 1、5 或 60 分钟;使用接触式触针表面轮廓仪(SSP)和非接触式聚焦变化 3D 显微镜(FVM)测量 Ra。使用微 pH 传感器测量表面 pH 值。数据在 alpha=0.05 的显著性水平上进行分析。SSP 和 FVM 之间的 Ra 存在显著相关性。FVM 图像显示,绿茶暴露不同时间后,表面形态没有变化。与可乐和橙汁不同,绿茶暴露对 Ra 或 pH 值没有显著影响。暴露于饮料后,表面 pH 值与 Ra 变化之间存在显著相关性。光学表面分析和微 pH 传感器可能是用于非破坏性、定量评估软饮料对牙釉质侵蚀的有用工具。