Division of Removable Prosthetics, Department of Oral and Maxillofacial Rehabilitation, Kanagawa Dental College, Yokosuka, Kanagawa, Japan.
Dent Mater J. 2012;31(3):472-80. doi: 10.4012/dmj.2011-237. Epub 2012 May 14.
The purpose of our study was to evaluate the effects of surface modifications on the bond strength between veneering porcelains and Yttria-stabilized tetragonal zirconia (Y-TZP). In a bond strength tests, the effect of control, 70 µm alumina-sandblasting, 30 µm and 110 µm silica-coating of the Y-TZP surface on bonding were evaluated with veneering porcelains. In addition, the effect of surface modification on the flexural strength of Y-TZP was also evaluated. The data was analyzed using one-way ANOVA and Tukey test. All specimens showed bond strength values in excess of 25 MPa, the minimum allowed by ISO9693. In addition, significantly differences were found between the control and the 30 µm silica-coated. On the other hand the flexural strength of Y-TZP does not significantly difference for any surface modification. These results indicate that silica-coating may provide an effective pre-treatment for this enhancement of the bond strength while maintaining the strength of Y-TZP.
我们研究的目的是评估表面改性对饰面瓷与氧化钇稳定四方氧化锆(Y-TZP)之间结合强度的影响。在结合强度测试中,评估了控制组、70μm氧化铝喷砂、30μm和 110μm 二氧化硅涂层对 Y-TZP 表面与饰面瓷结合的影响。此外,还评估了表面改性对 Y-TZP 弯曲强度的影响。数据采用单因素方差分析和 Tukey 检验进行分析。所有样本的结合强度值均超过 25MPa,符合 ISO9693 的最低要求。此外,控制组和 30μm 二氧化硅涂层之间存在显著差异。另一方面,对于任何表面改性,Y-TZP 的弯曲强度均无显著差异。这些结果表明,二氧化硅涂层可为提高结合强度提供有效预处理,同时保持 Y-TZP 的强度。