复合树脂修复体周围的微间隙和脱矿进展。

Microgaps and Demineralization Progress around Composite Restorations.

机构信息

Operative Dentistry Division, Conservative Dental Sciences, King Abdulaziz University, Jeddah, Saudi Arabia Cariology and Operative Dentistry Department, Graduate School of Medical and Dental Sciences, Tokyo Medical and Dental University, Tokyo, Japan.

Cariology and Operative Dentistry Department, Graduate School of Medical and Dental Sciences, Tokyo Medical and Dental University, Tokyo, Japan.

出版信息

J Dent Res. 2015 Aug;94(8):1070-7. doi: 10.1177/0022034515589713. Epub 2015 Jun 16.

Abstract

This study investigated the influence of adhesives and marginal sealing on demineralization progress using optical coherence tomography (OCT). Cavities (4 × 2 mm) were prepared in bovine incisors and restored using Clearfil SE Protect (SP), Bond Force (BF), Scotchbond Universal (SB), or G-Bond Plus (GB), followed by Estelite Flow Quick flowable composite. The control group received no adhesive (n = 10). After 3-d incubation in artificial saliva and 10,000 thermal cycles, gaps at enamel and dentin margins were measured at 8 locations on cross-sectional images obtained from each restoration using swept-source OCT at 1310-nm wavelength. Specimens were demineralized using acidified gel (pH = 4.5) for 5 wk and scanned every week to monitor the lesion progress at the same marginal locations. Repeated-measures analysis of variance showed that demineralization period and adhesive type and their interaction had a significant effect on the lesion size in both substrates (P < 0.001). SP, BF, and SB had significantly lower enamel and dentin initial gaps than the control and GB (P < 0.05). Enamel lesion progress was slower in the fluoride-releasing adhesives SP and BF and significantly different from SB, GB, and the control (P < 0.001). SP and BF dentin lesions were significantly different from GB and the control (P < 0.001), but not from SB (P > 0.05). A significant positive correlation (P < 0.05) was found between initial gap length and formed lesion size in both substrates, which was stronger in enamel (r = 0.63) than dentin (r = 0.35). Microgaps forming at the margins of restorations depend on adhesives and significantly contribute to the progress of demineralization around the margins, while fluoride release may decrease the rate of progression.

摘要

本研究使用光相干断层扫描(OCT)研究了粘结剂和边缘密封对脱矿进展的影响。在牛切牙上制备(4×2mm)窝洞,使用 Clearfil SE Protect(SP)、Bond Force(BF)、Scotchbond Universal(SB)或 G-Bond Plus(GB)粘结剂,随后使用 Estelite Flow Quick 流动复合树脂修复。对照组不使用粘结剂(n=10)。在人工唾液中孵育 3 天后,经过 10000 次热循环,在每个修复体的横截面上获得的 1310nm 波长的扫频源 OCT 图像上,在 8 个位置测量牙釉质和牙本质边缘的间隙。使用酸化凝胶(pH=4.5)对标本进行 5 周脱矿处理,并每周扫描一次,以监测相同边缘位置的病变进展。重复测量方差分析显示,脱矿时间、粘结剂类型及其相互作用对两种基质中的病变大小均有显著影响(P<0.001)。SP、BF 和 SB 的牙釉质和牙本质初始间隙明显低于对照组和 GB(P<0.05)。含氟释放粘结剂 SP 和 BF 的牙釉质病变进展较慢,与 SB、GB 和对照组明显不同(P<0.001)。SP 和 BF 的牙本质病变明显不同于 GB 和对照组(P<0.001),但与 SB 无差异(P>0.05)。在两种基质中,初始间隙长度与形成的病变大小之间均存在显著正相关(P<0.05),牙釉质中的相关性更强(r=0.63),牙本质中的相关性较弱(r=0.35)。修复体边缘形成的微间隙取决于粘结剂,并且显著促进边缘周围的脱矿进展,而氟化物释放可能会降低进展速度。