Abstract

AIM

This study was carried out to evaluate and compare solubility and microleakage of the newly introduced moisture tolerant glass carbomer sealant.

STUDY DESIGN

For evaluation of solubility, 20 specimens of glass carbomer and conventional glass ionomer were prepared and immersed in artificial saliva of pH 4 and 6 for seven days. The difference between initial and final weight was calculated. For evaluation of microleakage, glass carbomer was compared with a conventional resin sealant. 20 premolar teeth indicated for orthodontic extraction were collected and divided into two groups and the respective sealants were applied. It was subjected to thermocycling and then kept immersed in methylene blue for 24 hours. Dye penetration was scored.

RESULTS

The glass carbomer specimens were less soluble than the conventional glass ionomer at both pH values. There was no significant difference in the microleakage.

CONCLUSION

Being moisture resistant, glass carbomer can be used as an alternative fissure sealant material; especially in young children with partially erupted teeth and where obtaining moisture control is difficult.

摘要

目的

本研究旨在评估和比较新推出的耐湿性玻璃卡波姆封闭剂的溶解性和微渗漏情况。

研究设计

为评估溶解性,制备了20个玻璃卡波姆和传统玻璃离子体标本,并将其浸泡在pH值为4和6的人工唾液中7天。计算初始重量和最终重量之间的差异。为评估微渗漏情况,将玻璃卡波姆与传统树脂封闭剂进行比较。收集20颗因正畸需要拔除的前磨牙,分为两组并分别应用相应的封闭剂。对其进行热循环处理,然后在亚甲蓝中浸泡24小时。对染料渗透情况进行评分。

结果

在两个pH值下,玻璃卡波姆标本的溶解性均低于传统玻璃离子体。微渗漏方面无显著差异。

结论

由于具有耐湿性,玻璃卡波姆可作为一种替代的窝沟封闭剂材料;尤其适用于牙齿部分萌出的幼儿以及难以控制湿度的情况。