Abstract

BACKGROUND

The effect of bleaching on enamel surfaces, as well as exploring methods of preventing the weakening of bond strength of two different adhesives to bleached enamel surfaces.

OBJECTIVE

This study compared the shear bond strength (SBS) of two different adhesives on bleached enamel immediately after bleaching, with a 1-week delay, and following application of an antioxidizing agent after bleaching. Materilas and Method: The enamel surfaces of 140 incisors were divided into 14 groups. Two unbleached enamel groups (n = 20) were prepared as negative controls of the Adper Single Bond 2 total-etch and Clearfil Tri S Bond self-etch adhesives. The remaining surfaces were randomly divided into two bleaching groups treated with 35% Beyond Max (n = 60) and 38% Opalescence Xtra Boost (n = 60). Each bleaching group was then divided into two subgroups using the total and self-etch adhesive systems. Specimens were bonded immediately after bleaching, after treatment with 10% sodium ascorbate (SA) gel, or after 1-week of immersion in artificial saliva. All groups were restored with composite resin. After thermocycling, SBS was measured and data were analyzed.

RESULTS

In the control groups, there was no statistically-significant difference in SBS between self-and total-etch adhesives. Among all bleaching groups, no statistically-significant differences in SBS were noted, although the SA-treated delayed bonding (1-week) groups had the highest values. The lowest values were noted for the groups bonded immediately after bleaching.

摘要

背景

漂白对牙釉质表面的影响,以及探索防止两种不同粘合剂与漂白牙釉质表面结合强度减弱的方法。

目的

本研究比较了两种不同粘合剂在漂白后立即、延迟1周以及漂白后使用抗氧化剂后的漂白牙釉质上的剪切粘结强度(SBS)。材料与方法:140颗切牙的牙釉质表面分为14组。制备两个未漂白牙釉质组(n = 20)作为Adper Single Bond 2全蚀刻和Clearfil Tri S Bond自蚀刻粘合剂的阴性对照。其余表面随机分为两组,分别用35% Beyond Max(n = 60)和38% Opalescence Xtra Boost(n = 60)进行漂白处理。然后,每个漂白组使用全蚀刻和自蚀刻粘合剂系统再分为两个亚组。标本在漂白后立即、用10%抗坏血酸钠(SA)凝胶处理后或在人工唾液中浸泡1周后进行粘结。所有组均用复合树脂修复。热循环后,测量SBS并分析数据。

结果

在对照组中,自蚀刻和全蚀刻粘合剂之间的SBS没有统计学上的显著差异。在所有漂白组中,SBS没有统计学上的显著差异,尽管SA处理的延迟粘结(1周)组的值最高。漂白后立即粘结的组的值最低。