Int J Oral Maxillofac Implants. 2020 Sep/Oct;35(5):948-954. doi: 10.11607/jomi.8224.
The aim of this study was to compare the effect of different surface treatments applied to short titanium and zirconia abutments on the bond strength of single-unit zirconia crowns.
Sixty titanium abutments were shortened to 3 mm in length, fixed to analogs, and embedded in acrylic blocks. Three-dimensional views of abutments were obtained by scanning; then, zirconia abutments and copings were produced. The samples, which included titanium (n = 60) and zirconia (n = 60) abutments, were divided into five different groups (n = 12), and surface treatments were carried out; 1.5-W and 3-W Er,Cr:YSGG laser treatment, ALO sandblasting, and tribochemical silica coating were applied to the groups, and the control group had no surface treatment. Copings were cemented to the samples with self-adhesive resin cement. The samples were then subjected to the pull-out test, and the results were processed via statistical analysis.
There was a significant difference between the titanium and zirconia groups (P < .001). The mean bond strength values of the titanium samples were higher than those of the zirconia samples. The tribochemical silica coating gave a higher bond strength than the other treatments when applied to titanium abutments. For the zirconia abutments, the 1.5-W laser treatment, 3-W laser treatment, tribochemical silica coating, and AlO sandblasting groups differed significantly from the control group; however, they were not significantly different from each other.
The bond strength of zirconia crowns to short titanium and zirconia abutments increases with surface treatments. Furthermore, the surface treatments were more effective in increasing the bond strength for the titanium abutments than for the zirconia abutments.
本研究旨在比较应用于短钛和氧化锆基台的不同表面处理方法对单颗氧化锆冠粘结强度的影响。
将 60 个钛基台缩短至 3mm 长度,固定在模型上,并嵌入丙烯酸块中。通过扫描获得基台的三维视图;然后,制作氧化锆基台和修复体。将包括钛(n=60)和氧化锆(n=60)基台的样本分为五组(n=12),并进行表面处理;分别采用 1.5-W 和 3-W Er,Cr:YSGG 激光处理、ALO 喷砂处理和化学机械硅涂层处理,对照组不进行表面处理。用自粘结树脂水门汀将修复体粘结到样本上。然后对样本进行拔出试验,并对结果进行统计分析。
钛和氧化锆组之间存在显著差异(P<.001)。钛样本的平均粘结强度值高于氧化锆样本。与其他处理方法相比,将化学机械硅涂层应用于钛基台时,可获得更高的粘结强度。对于氧化锆基台,1.5-W 激光处理、3-W 激光处理、化学机械硅涂层处理和 ALO 喷砂处理组与对照组有显著差异;但彼此之间无显著差异。
对短钛和氧化锆基台进行表面处理可提高氧化锆冠的粘结强度。此外,与氧化锆基台相比,表面处理方法更能有效提高钛基台的粘结强度。