Department of Prosthodontics, Institute of Dental Sciences, Siksha O' Anusandhan, Deemed to be University, Bhubaneswar, Odisha, India.
Department of Prosthodontics, College of Dentistry, Jazan University, Saudi Arabia.
Ann Afr Med. 2021 Apr-Jun;20(2):116-120. doi: 10.4103/aam.aam_30_20.
Clinically, adhesion failure is the most critical problem because of the failure of the optimal bond between denture base and the soft liner.
This study was performed to assess the tensile bond strength of two temporary soft liners to different denture base resins.
Forty-eight blocks with 16 samples each of heat-cured denture base resin of three different types were fabricated from custom-made stainless steel die after de-waxing mold space. Surface roughening of each acrylic resin specimens which bonds with soft liners was done by abrading the surface and to this temporary soft liners (Perma soft denture liner and Pro soft denture liner) were bonded. The universal testing machine was used to test the tensile strength of bonded space. The results were statistically analyzed using the Statistical Software IBM SPSS Statistics for Windows, version 20.0. (Armonk, NY, USA: IBM Corp.) using the Chi-square test, Post hoc Tukey's HSD, and two way ANOVA tests.
It was observed that Perma soft was prevalent over Pro-soft denture liner on the basis of tensile bond strength with all three different types of denture base resins. Trevalon HI and acrylic composite exhibited better bond strength results with both Perma soft and GC Pro-soft denture liner as compared to other types of denture base resins.
Perma soft had a better bond strength compared to Pro-soft denture liner in bonding modified denture base and conventional resins.
临床上,黏附失败是最关键的问题,因为义齿基托和软衬之间的最佳黏附失败了。
本研究旨在评估两种临时软衬材料与不同义齿基托树脂的拉伸黏附强度。
从定制的不锈钢模具中去除蜡模空间后,用三种不同类型的热凝义齿基托树脂制作了 48 个块,每个块有 16 个样本。用磨料打磨每个与软衬结合的丙烯酸树脂样本的表面,然后将临时软衬(Perma soft 义齿衬垫和 Pro soft 义齿衬垫)与样本结合。使用万能试验机测试黏合空间的拉伸强度。使用 IBM SPSS Statistics for Windows 版本 20.0(美国纽约州阿蒙克:IBM 公司)统计软件对结果进行统计分析,使用卡方检验、事后 Tukey HSD 检验和双向 ANOVA 检验。
观察到,在三种不同类型的义齿基托树脂中,Perma soft 在拉伸黏附强度方面均优于 Pro-soft 义齿衬垫。与其他类型的义齿基托树脂相比,Trevailon HI 和丙烯酸复合材料与 Perma soft 和 GC Pro-soft 义齿衬垫都显示出更好的黏附强度。
Perma soft 与 Pro-soft 义齿衬垫相比,在改性义齿基托和常规树脂的黏附方面具有更好的黏附强度。