一种玻璃离子水门汀黏固剂的评估:细菌渗漏

An evaluation of a glass ionomer luting agent: bacterial leakage.

作者信息

Fitzgerald M, Heys R J, Heys D R, Charbeneau G T

出版信息

J Am Dent Assoc. 1987 Jun;114(6):783-6. doi: 10.14219/jada.archive.1987.0168.

Abstract

This study quantitatively evaluates the bacterial leakage beneath crowns cemented with a glass ionomer cement compared with those cemented with a polycarboxylate cement or a varnish plus zinc phosphate cement. Bacterial samples were taken from beneath full crowns cemented with the test luting agents 3, 10, and 56 days after cementation. Two-way analysis of variance of the resultant data showed a significant increase in bacterial counts for zinc phosphate, a significant decrease for polycarboxylate, and no change for glass ionomer. These findings suggest that bacterial leakage may not be the reason for the reported poor clinical response associated with glass ionomer luting agents.

摘要

本研究定量评估了用玻璃离子水门汀粘结的全冠下方的细菌渗漏情况,并与用聚羧酸锌水门汀或清漆加磷酸锌水门汀粘结的全冠进行了比较。在粘结后3天、10天和56天,从用测试粘结剂粘结的全冠下方采集细菌样本。对所得数据进行的双向方差分析表明,磷酸锌组的细菌计数显著增加,聚羧酸锌组显著减少,玻璃离子组无变化。这些发现表明,细菌渗漏可能不是报道的与玻璃离子粘结剂相关的临床反应不佳的原因。

相似文献

2
Leakage of various types of luting agents.各类粘结剂的渗漏。
J Prosthet Dent. 1991 Dec;66(6):763-6. doi: 10.1016/0022-3913(91)90411-o.

文献AI研究员

20分钟写一篇综述,助力文献阅读效率提升50倍。

立即体验

用中文搜PubMed

大模型驱动的PubMed中文搜索引擎

马上搜索

文档翻译

学术文献翻译模型,支持多种主流文档格式。

立即体验