Aoyama Sota, Kubo Yunosuke, Sok Ratnak, Kusaka Jin
Propulsion and Energy Systems Laboratory, Waseda University, 3-4-1 Okubo, Shinjuku, Tokyo, 169-8555, Japan.
Heliyon. 2024 Feb 20;10(4):e26592. doi: 10.1016/j.heliyon.2024.e26592. eCollection 2024 Feb 29.
This work investigates oxygen-storage capacity (OSC) changes during thermal degradation in modern three-way catalysts. Two experiments are performed using catalysts with different degradation degrees to evaluate OSC and reaction rates. The CO production test, where CO and O are supplied at a constant temperature, shows decreased CO production with more degraded catalysts and reduced purification. The CO production test is conducted using transient temperature increases, showing that the maximum CO production temperature increases with catalyst degradation. The results reveal an increase in activation energy in the oxygen desorption reaction caused by thermal degradation progresses and a decrease in OSC, resulting in temperature increases in the oxygen storage reaction. In the surface reaction and mass transport model considering the 30 elementary reactions, the predicted results are well-validated for CO production, enabling good oxygen storage predictions based on actual data. These results can be used to predict OSC by formulating the changes in active site density and activation energy due to degradation.