Mierzejewska Żaneta Anna, Łukaszuk Kamila, Rusztyn Bartłomiej, Maliszewski Kacper
Institute of Biomedical Engineering, Faculty of Mechanical Department, Bialystok University of Technology, 15-351 Bialystok, Poland.
Department of Maxillofacial and Plastic Surgery, Medical University of Bialystok, 15-089 Białystok, Poland.
J Funct Biomater. 2025 May 23;16(6):193. doi: 10.3390/jfb16060193.
The aim of this study was to evaluate the effect of different bleaching protocols, including laser-assisted techniques, on the microhardness, surface roughness, and tribological resistance of selected light-cured composites. Three Estelite Universal Flow composites with different flow properties and G-aenial Universal Flo composites were tested. Each group underwent bleaching procedures using Opalescence agents at 10%, 16%, and 40% concentrations, with and without laser activation. Surface microhardness was assessed using the Vickers method, roughness was measured with 3D confocal laser microscopy, and friction coefficients and wear patterns were evaluated using tribological testing. All bleaching protocols resulted in reduced microhardness and increased surface roughness. The most significant changes were observed after treatment with 40% hydrogen peroxide. Laser application, particularly at 16% concentration of carbamide peroxide, helped to partially mitigate these effects in some materials. Bleaching procedures, especially those involving high peroxide concentrations, significantly deteriorated the surface properties of dental composites, which may have clinical implications for the patients.
本研究的目的是评估不同漂白方案(包括激光辅助技术)对所选光固化复合材料的显微硬度、表面粗糙度和摩擦学阻力的影响。测试了三种具有不同流动性能的Estelite Universal Flow复合材料和G-aenial Universal Flo复合材料。每组使用浓度为10%、16%和40%的Opalescence试剂进行漂白程序,有或没有激光激活。使用维氏方法评估表面显微硬度,用三维共聚焦激光显微镜测量粗糙度,并使用摩擦学测试评估摩擦系数和磨损模式。所有漂白方案均导致显微硬度降低和表面粗糙度增加。在用40%过氧化氢处理后观察到最显著的变化。激光应用,特别是在16%浓度的过氧化脲时,有助于部分减轻某些材料中的这些影响。漂白程序,尤其是那些涉及高浓度过氧化物的程序,显著恶化了牙科复合材料的表面性能,这可能对患者具有临床意义。