Hamanishi C, Kitamoto K, Tanaka S, Otsuka M, Doi Y, Kitahashi T
Department of Orthopaedic Surgery, Kinki University School of Medicine, Osaka, Japan.
J Biomed Mater Res. 1996 Fall;33(3):139-43. doi: 10.1002/(SICI)1097-4636(199623)33:3<139::AID-JBM3>3.0.CO;2-R.
Vancomycin (VCM), a methiciline-cefem resistant Staphylococcus aureus (MRSA)-specific antibiotic, was incorporated in a self-setting tetracalcium phosphate (TTCP)-dicalcium phosphate dihydrate (DCPD) apatite cement that hardened isothermally into a hydroxyapatite (HAP) phase with crystallinity similar to that of host bone. Effective release of VCM into PBS lasted for 2 weeks from cements containing 1% VCM and for longer than 9 weeks from cements containing 5% VCM. The rate of release of VCM differed between cements with different crystallinities as well as between the two dissolution media, PBS and simulated body fluid. Mean concentration of VCM in the bone marrow tissue released from cements containing 5% VCM was 20 times the minimum inhibitory concentration 3 weeks after implantation in bone. Direct contact with new bone was observed with the cements containing 1% VCM. Slow delivery of VCM from a self-setting TTCP-DCPD apatite cement with low crystallinity could be used to treat MRSA osteomyelitis.
万古霉素(VCM)是一种对耐甲氧西林头孢菌素金黄色葡萄球菌(MRSA)具有特异性的抗生素,被掺入一种自固化磷酸四钙(TTCP)-二水磷酸二钙(DCPD)磷灰石骨水泥中,该骨水泥在等温条件下硬化为与宿主骨结晶度相似的羟基磷灰石(HAP)相。从含1%VCM的骨水泥中,VCM在磷酸盐缓冲盐水(PBS)中的有效释放持续2周,而从含5%VCM的骨水泥中,有效释放持续超过9周。不同结晶度的骨水泥以及两种溶解介质(PBS和模拟体液)中VCM的释放速率有所不同。含5%VCM的骨水泥植入骨中3周后,骨髓组织中VCM的平均浓度是最低抑菌浓度的20倍。观察到含1%VCM的骨水泥与新骨直接接触。低结晶度的自固化TTCP-DCPD磷灰石骨水泥缓慢释放VCM可用于治疗MRSA骨髓炎。