Suppr超能文献

用碱法和碱性过氧化物法从大麦秸秆中分离出的木质素的分级和结构表征

Fractional and structural characterization of lignins isolated by alkali and alkaline peroxide from barley straw.

作者信息

Sun R C, Sun X F, Wen J L

机构信息

State Key Laboratory of Pulp and Paper Engineering, College of Paper and Environment Engineering, South China University of Technology, Guangzhou 510640, People's Republic of China.

出版信息

J Agric Food Chem. 2001 Nov;49(11):5322-30. doi: 10.1021/jf010645y.

Abstract

A sequential treatment of dewaxed barley straw with sodium hydroxide, different concentrations of hydrogen peroxide, and potassium hydroxide/sodium borate degraded various proportions of the original lignin and solubilized different amounts of the original hemicelluloses. The isolated lignin fractions were subjected to comprehensive structural characterization by UV, FT-IR, and (13)C NMR spectroscopy, and their chemical compositions were analyzed by alkaline nitrobenzene oxidation. All of the lignin fractions were typical of grass lignins and had weight-average molecular weights between 1750 and 2190. It was found that the peroxide treatment at low concentrations (< or =2.0%) resulted in a slight increase in the amount of carboxyl groups, whereas the treatment at a relatively high concentration of alkaline peroxide, such as at 3.0% H(2)O(2), led to a noticeable oxidation of the lignins, as shown by an increase of carboxyl groups. Moreover, the results obtained indicated that the successive treatments with alkali and alkaline peroxide under the conditions used did not significantly affect the beta-O-4 structures of lignins. Substantial amounts of etherified ferulic acids were cleaved by the sequential treatments with alkaline peroxide, as shown in the (13)C NMR spectra. The results underscore the structural differences between alkali- and alkaline peroxide-soluble lignins from barley straw.

摘要

用氢氧化钠、不同浓度的过氧化氢以及氢氧化钾/硼酸钠对脱蜡大麦秸秆进行顺序处理,降解了不同比例的原始木质素,并溶解了不同量的原始半纤维素。对分离得到的木质素组分进行了紫外光谱、傅里叶变换红外光谱和(13)C核磁共振光谱的综合结构表征,并通过碱性硝基苯氧化分析了它们的化学组成。所有木质素组分均为典型的禾本科木质素,重均分子量在1750至2190之间。研究发现,低浓度(≤2.0%)的过氧化物处理会使羧基数量略有增加,而在相对高浓度的碱性过氧化物(如3.0% H₂O₂)处理下,木质素会发生明显氧化,表现为羧基数量增加。此外,所得结果表明,在所使用的条件下,碱和碱性过氧化物的连续处理对木质素的β-O-4结构没有显著影响。如(13)C核磁共振光谱所示,大量醚化阿魏酸在碱性过氧化物的顺序处理中被裂解。这些结果突出了大麦秸秆中碱溶性和碱性过氧化物溶性木质素之间的结构差异。