Baratieri Luiz Narciso, Machado Adriana, Van Noort Richard, Ritter André V, Baratieri Naira Maria Mascarenhas
Department of Operative Dentistry, Universidade Federal de Santa Catarina, Florianópolis, Brazil.
Oper Dent. 2002 Jul-Aug;27(4):319-24.
This study evaluated the influence of the pulp protection technique on clinical performance of amalgam restorations after three years, with particular reference to post-operative sensitivity and secondary caries. One hundred and twenty (120) Class II amalgam restorations (68 premolars, 52 molars; 78 MOD, 42 OD/MO) were placed in 30 participants (four restorations per participant). The restorations were divided into four groups according to the pulp protection technique used: copal varnish; 2% neutral sodium fluoride; adhesive resin and no pulp protection. The parameters evaluated were post-operative sensitivity, staining of the dental structure, tooth vitality, partial or total loss of the restoration and secondary caries. One hundred and eight (108) restorations were available for evaluation after three years. No partial or total loss of restorations had occurred; all teeth were vital, no tooth structure staining or secondary caries was detected in any of the restored teeth. Post-operative sensitivity was observed only in two restorations at baseline and at seven-days. The three-year clinical performance of teeth restored with a high copper dispersed phase amalgam was not affected by the choice of pulp protection technique.
本研究评估了牙髓保护技术对银汞合金修复体三年后临床性能的影响,特别涉及术后敏感性和继发龋。120个II类银汞合金修复体(68个前磨牙,52个磨牙;78个MOD,42个OD/MO)被放置在30名参与者口中(每位参与者4个修复体)。根据所使用的牙髓保护技术,修复体被分为四组:松香清漆;2%中性氟化钠;粘结树脂和无牙髓保护。评估的参数包括术后敏感性、牙体结构染色、牙齿活力、修复体部分或全部丧失以及继发龋。三年后有108个修复体可供评估。没有发生修复体部分或全部丧失的情况;所有牙齿均有活力,在任何一颗修复牙齿中均未检测到牙体结构染色或继发龋。仅在基线和七天时在两个修复体中观察到术后敏感性。高铜分散相银汞合金修复牙齿的三年临床性能不受牙髓保护技术选择的影响。