Suppr超能文献

将硫酸铅矿(PbSO₄)和废旧汽车电池中的铅废料生物转化为方铅矿(PbS)。

Biological conversion of anglesite (PbSO(4)) and lead waste from spent car batteries to galena (PbS).

作者信息

Weijma Jan, De Hoop Klaas, Bosma Wobby, Dijkman Henk

机构信息

Sub-department Environmental Technology, Bomenweg 2, Wageningen University, 6700 EV, Wageningen, The Netherlands.

出版信息

Biotechnol Prog. 2002 Jul-Aug;18(4):770-5. doi: 10.1021/bp025523k.

Abstract

Lead paste, a solid mixture containing PbSO(4), PbO(2), PbO/Pb(OH)(2) precipitate, and elemental Pb, is one of the main waste fractions from spent car batteries. Biological sulfidation represents a new process for recovery of lead from this waste. In this process the lead salts in lead paste are converted to galena (PbS) by sulfate-reducing bacteria. This paper investigates a continuous process for sulfidation of anglesite (PbSO(4)), the main constituent of lead paste, and lead paste, consisting of a laboratory-scale gas-lift bioreactor to which a slurry of anglesite or lead paste was supplied. Sulfate or elemental sulfur was added as an additional sulfur source. Hydrogen gas served as an electron donor for the biological reduction of sulfate and elemental sulfur to sulfide by sulfate- and sulfur-reducing bacteria. Anglesite was almost completely converted to galena at a loading rate of 19 kg of PbSO(4) m(-)(3) day(-)(1), producing a sludge of which the crystalline lead phases consisted of >98% PbS (galena) and 1-2% elemental Pb. With lead paste, stable sulfidation rates of up to 17 kg of lead paste m(-)(3) day(-)(1) were demonstrated, producing a sludge of which the crystalline lead phases consisted of an estimated >96% PbS, 1-2% elemental Pb, and 1-2% PbO(2).

摘要

铅膏是一种含有硫酸铅(PbSO₄)、二氧化铅(PbO₂)、氧化铅/氢氧化铅(PbO/Pb(OH)₂)沉淀和单质铅的固体混合物,是废旧汽车电池的主要废渣之一。生物硫化是一种从这种废渣中回收铅的新工艺。在这个过程中,铅膏中的铅盐通过硫酸盐还原菌转化为方铅矿(PbS)。本文研究了一种连续工艺,用于硫化铅膏的主要成分硫酸铅矿(PbSO₄)和铅膏,该工艺包括一个实验室规模的气升式生物反应器,向其中供应硫酸铅矿或铅膏的浆料。添加硫酸盐或单质硫作为额外的硫源。氢气作为电子供体,通过硫酸盐还原菌和硫还原菌将硫酸盐和单质硫生物还原为硫化物。在装载速率为19 kg PbSO₄ m⁻³ day⁻¹时,硫酸铅矿几乎完全转化为方铅矿,产生的污泥中结晶铅相由>98%的PbS(方铅矿)和1 - 2%的单质铅组成。对于铅膏,稳定的硫化速率高达17 kg铅膏 m⁻³ day⁻¹,产生的污泥中结晶铅相估计由>96%的PbS、1 - 2%的单质铅和1 - 2%的PbO₂组成。