Leitner V M, Marschütz M K, Bernkop-Schnürch A
Institute of Pharmaceutical Technology and Biopharmaceutics, Centre of Pharmacy, University of Vienna, Althanstr 14, A-1090, Vienna, Austria.
Eur J Pharm Sci. 2003 Jan;18(1):89-96. doi: 10.1016/s0928-0987(02)00245-2.
The objective of this study was to evaluate the influence of the molecular mass and accordingly the polymer chain length on mucoadhesion and cohesion of thiolated polymers. Linear poly(acrylic acid)-cysteine (PAA-Cys) conjugates of 2-, 45-, 250- and 450 kDa (PAA(2)-Cys, PAA(45)-Cys, PAA(250)-Cys and PAA(450)-Cys) and polycarbophil-cysteine (PCP-Cys, 750-3000 kDa), all displaying on average 404.1+/-65.5 microMol thiol groups per gram polymer were compressed into tablets to perform disintegration tests, mucoadhesion studies and viscosity measurements. Moreover, the influence of free unbound cysteine on mucoadhesion was evaluated. Disintegration tests showed a stability of the tablets as following: PAA(2)-Cys<PAA(45)-Cys<PAA(250)-Cys<PAA(450)-Cys=PCP-Cys. According to tensile studies and tests on the rotating cylinder the following rank order in mucoadhesive properties could be established: PAA(2)-Cys<PAA(45)-Cys<PCP-Cys<PAA(250)-Cys<PAA(450)-Cys. Evidence for the formation of disulphide bonds between thiolated polymers and mucin could be provided by the addition of free cysteine resulting in strongly decreased mucoadhesion and by viscosity studies showing comparatively higher viscosity of conjugate/mucin mixtures than of unthiolated polymer/mucin mixtures. The results of the present study contribute to the development of new polymers displaying further improved mucoadhesive properties.
本研究的目的是评估分子质量以及相应的聚合物链长度对硫醇化聚合物的粘膜粘附性和内聚性的影响。将平均每克聚合物含有404.1±65.5微摩尔硫醇基团的2 kDa、45 kDa、250 kDa和450 kDa的线性聚(丙烯酸)-半胱氨酸(PAA-Cys)共轭物(PAA(2)-Cys、PAA(45)-Cys、PAA(250)-Cys和PAA(450)-Cys)以及聚卡波非-半胱氨酸(PCP-Cys,750 - 3000 kDa)压制成片剂,以进行崩解试验、粘膜粘附性研究和粘度测量。此外,还评估了游离未结合半胱氨酸对粘膜粘附性的影响。崩解试验表明片剂的稳定性如下:PAA(2)-Cys < PAA(45)-Cys < PAA(250)-Cys < PAA(450)-Cys = PCP-Cys。根据拉伸研究和旋转圆筒试验,可以确定粘膜粘附性能的以下排序:PAA(2)-Cys < PAA(45)-Cys < PCP-Cys < PAA(250)-Cys < PAA(450)-Cys。游离半胱氨酸的加入导致粘膜粘附性显著降低,以及粘度研究表明共轭物/粘蛋白混合物的粘度相对高于未硫醇化聚合物/粘蛋白混合物的粘度,这可以为硫醇化聚合物与粘蛋白之间形成二硫键提供证据。本研究结果有助于开发具有进一步改善的粘膜粘附性能的新型聚合物。