Albarghouthi Methal N, Stein Thomas M, Barron Annelise E
Department of Chemical Engineering, Northwestern University, Evanston, IL 60208, USA.
Electrophoresis. 2003 Apr;24(7-8):1166-75. doi: 10.1002/elps.200390150.
We present the polymer poly-N-hydroxyethylacrylamide (PHEA) (polyDuramide) as a novel, hydrophilic, adsorbed capillary coating for electrophoretic protein analysis. Preparation of the PHEA coating requires a simple and fast (30 min) protocol that can be easily automated in capillary electrophoresis instruments. Over the pH range of 3-8.4, the PHEA coating is shown to reduce electroosmotic flow (EOF) by about 2 orders of magnitude compared to the bare silica capillary. In a systematic comparative study, the adsorbed PHEA coating exhibited minimal interactions with both acidic and basic proteins, providing efficient protein separations with excellent reproducibility on par with a covalent polyacrylamide coating. Hydrophobic interactions between proteins and a relatively hydrophobic poly-N,N-dimethylacrylamide (PDMA) adsorbed coating, on the other hand, adversely affected separation reproducibility and efficiency. Under both acidic and basic buffer conditions, the adsorbed PHEA coating produced an EOF suppression performance comparable to that of covalent polyacrylamide coating and superior to that of adsorbed PDMA coating. The protein separation performance in PHEA-coated capillaries was retained for 275 consecutive protein separation runs at pH 8.4, and for more than 800 runs at pH 4.4. The unique and novel combination of hydrophilicity and adsorptive coating ability of PHEA makes it a suitable wall coating for automated microscale analysis of proteins by capillary array systems.
我们提出将聚合物聚-N-羟乙基丙烯酰胺(PHEA)(聚杜拉酰胺)作为一种用于电泳蛋白质分析的新型亲水性吸附毛细管涂层。制备PHEA涂层需要一个简单快速(30分钟)的方案,该方案可在毛细管电泳仪器中轻松实现自动化。在pH值为3-8.4的范围内,与裸露的硅胶毛细管相比,PHEA涂层可将电渗流(EOF)降低约2个数量级。在一项系统的对比研究中,吸附的PHEA涂层与酸性和碱性蛋白质的相互作用最小,能够实现高效的蛋白质分离,且具有与共价聚丙烯酰胺涂层相当的出色重现性。另一方面,蛋白质与相对疏水的吸附性聚-N,N-二甲基丙烯酰胺(PDMA)涂层之间的疏水相互作用对分离的重现性和效率产生了不利影响。在酸性和碱性缓冲条件下,吸附的PHEA涂层产生的EOF抑制性能与共价聚丙烯酰胺涂层相当,且优于吸附的PDMA涂层。在pH 8.4时,PHEA涂层毛细管中的蛋白质分离性能在连续275次蛋白质分离运行中得以保持,在pH 4.4时则可保持800多次运行。PHEA独特的亲水性和吸附涂层能力的新颖组合使其成为毛细管阵列系统对蛋白质进行自动化微尺度分析的合适壁涂层。