Krajewski A, Ravaglioli A, Tinti A, Taddei P, Mazzocchi M, Martinetti R, Fagnano C, Fini M
ISTEC-CNR, Via Granarolo 64, 48018, Faenza (Ravenna), Italy.
J Mater Sci Mater Med. 2005 Feb;16(2):119-28. doi: 10.1007/s10856-005-5913-y.
Two bioactive silica-phosphate glasses, AP40 and RKKP, were compared in their behaviour in simulated biological environment. Their chemical composition is practically identical, except that RKKP contains small amounts of amphoteric network-former oxides Ta2O5 and La2O3 (composition in wt% for AP40: beta-Ca3(PO4)2 24.50, SiO2 44.30, CaO 18.60, Na2O 4.60, K2O 0.19, MgO 2.82, CaF2 4.99; RKKP: beta-Ca3(PO4)2 24.23, SiO2 43.82, CaO 18.40, Na2O 4.55, K2O 0.19, MgO 2.79, CaF2 4.94, Ta2O5 0.99, La2O3 0.09). Previous investigations showed a better performance in osteopenic bone for RKKP. To gain more insight into these differences in biological behaviour, the in vitro bioactivity of the glasses was studied by treatment with a continuously replenished Hanks' Balanced Salt Solution (HBSS). The glasses were examined before and after HBSS treatment for 20 and 40 days by X-ray Diffraction (XRD), Scanning Electron Microscopy (SEM), X-ray Energy Dispersion (EDX), Raman and IR vibrational spectroscopies. Some slight but notable differences between the two glasses were observed after HBSS treatment. IR and EDX analyses showed that deposits formed on both glasses were composed of a calcium deficient carbonate-apatite; however, the layer formed on RKKP glass was found to be slightly more calcium deficient and thinner. EDX analysis evidenced the presence of a small percentage of F- ions only in the layers formed on the RKKP samples. The differences disclosed, although slight, can contribute to the understanding of the different biological behaviour previously observed.
比较了两种生物活性硅磷酸盐玻璃AP40和RKKP在模拟生物环境中的行为。它们的化学成分几乎相同,只是RKKP含有少量两性网络形成氧化物Ta2O5和La2O3(AP40的重量百分比组成:β-Ca3(PO4)2 24.50,SiO2 44.30,CaO 18.60,Na2O 4.60,K2O 0.19,MgO 2.82,CaF2 4.99;RKKP:β-Ca3(PO4)2 24.23,SiO2 43.82,CaO 18.40,Na2O 4.55,K2O 0.19,MgO 2.79,CaF2 4.94,Ta2O5 0.99,La2O3 0.09)。先前的研究表明RKKP在骨质减少的骨骼中表现更好。为了更深入了解这些生物行为差异,通过用持续补充的汉克斯平衡盐溶液(HBSS)处理来研究玻璃的体外生物活性。通过X射线衍射(XRD)、扫描电子显微镜(SEM)、X射线能量色散(EDX)、拉曼光谱和红外振动光谱对玻璃在HBSS处理20天和40天前后进行了检查。HBSS处理后观察到两种玻璃之间存在一些细微但显著的差异。红外和EDX分析表明,在两种玻璃上形成的沉积物均由缺钙碳酸磷灰石组成;然而,发现RKKP玻璃上形成的层缺钙程度略高且更薄。EDX分析证明仅在RKKP样品上形成的层中存在少量F-离子。所揭示的差异虽然细微,但有助于理解先前观察到的不同生物行为。