Kim Jae-Pil, Yoon Tae-Ho, Mun Sung-Phil, Rhee Jong-Moon, Lee Jae-Suk
Korea Photonics Technology Institute, Bonchon-dong, Buk-gu, Gwangju 500-210, Republic of Korea.
Bioresour Technol. 2006 Feb;97(3):494-9. doi: 10.1016/j.biortech.2005.02.048.
Saw dust-reinforced linear low density polyethylene (LLDPE) (1:1) composites were prepared by using ethylene-vinyl alcohol copolymer (EVAL) as adhesion promoter to improve mechanical strength. To evaluate the optimum vinylalcohol (VA) content in EVAL, various EVAL samples containing different contents of VA were used. The tensile properties of saw dust-LLDPE composites were improved by using EVAL as adhesion promoter in place of ethylene-vinyl acetate copolymer (EVAc). The saw dust-LLDPE composites prepared with EVAL containing 15 mol% VA showed the maximum yield stress and modulus. The tensile stress increased with addition of EVAL up to 3wt% on the wood filler, and then leveled off in the range of 3-10 wt%. However, the elongation was decreased with increasing VA content. Hydrogen bonding interaction between saw dust and EVAL was detected by FT-IR spectra. When EVAL consisting with 15 mol% VA was used, good adhesion between saw dust and LLDPE matrix was confirmed by SEM fractography.
以乙烯-乙烯醇共聚物(EVAL)作为增粘剂,制备了锯末增强线性低密度聚乙烯(LLDPE)(1:1)复合材料,以提高其机械强度。为了评估EVAL中乙烯醇(VA)的最佳含量,使用了含有不同VA含量的各种EVAL样品。用EVAL代替乙烯-醋酸乙烯酯共聚物(EVAc)作为增粘剂,提高了锯末-LLDPE复合材料的拉伸性能。用含有15 mol% VA的EVAL制备的锯末-LLDPE复合材料表现出最大的屈服应力和模量。在木材填料上添加EVAL至3wt%时,拉伸应力增加,然后在3-10 wt%范围内趋于平稳。然而,伸长率随着VA含量的增加而降低。通过傅里叶变换红外光谱(FT-IR)检测到锯末与EVAL之间的氢键相互作用。当使用含有15 mol% VA的EVAL时,通过扫描电子显微镜(SEM)断口分析证实了锯末与LLDPE基体之间具有良好的粘附性。