Lakshminarayana G, Buddhudu S
Department of Physics, Sri Venkateswara University, Tirupati 517502, India.
Spectrochim Acta A Mol Biomol Spectrosc. 2005 Nov;62(1-3):364-71. doi: 10.1016/j.saa.2005.01.014.
A new series of heavy metal oxide (PbO) based zinc borate glasses in the chemical composition of (95-x)B(2)O(3)-5ZnO-xPbO (x=10, 15, 20, 25, 30, 35, 40, 45 and 50 mol%) have been prepared to verify their UV filtering performance. Both direct and indirect optical band gaps (E(opt)) have been evaluated for these glasses. For a reference glass of 45B(2)O(3)-5ZnO-50PbO, refractive indices at different wavelengths are measured and found the results satisfactorily correlated with the theoretical data upon the computation of Cauchy's constants of A=1.766029949, B=159531.024 nm(2) and C=-1.078 x 10(10) nm(4). Measurements concerning X-ray diffraction (XRD), FT-IR, differential scanning colorimeter (DSC) profiles have been carried out for this glass. The FT-IR profile has revealed that the glass has both BO(3) and BO(4) units. From DSC thermogram, glass transition temperature (T(g)), crystallization temperature (T(c)) and melting temperature (T(m)) have been located and from them, other related parameters of the glass have also been calculated. Visible absorption spectra of 45B(2)O(3)-5ZnO-(50-x)PbO-xCuO (x=0. 1, 0.2, 0.5 and 1.0 mol%) have revealed two absorption bands at around 400 nm ((2)B(1g)-->(2)E(g)) and 780 nm ((2)B(1g)-->(2)B(2g)) of Cu(2+) ions, respectively. Emission bands at 422 and 512 nm are found for the 1 mol % CuO doped glass with excitations at 306 and 332 nm.
已制备出一系列新的基于重金属氧化物(PbO)的硼酸锌玻璃,其化学组成为(95 - x)B₂O₃ - 5ZnO - xPbO(x = 10、15、20、25、30、35、40、45和50 mol%),以验证其紫外线过滤性能。已对这些玻璃评估了直接和间接光学带隙(E(opt))。对于45B₂O₃ - 5ZnO - 50PbO的参考玻璃,测量了不同波长下的折射率,发现计算出的柯西常数A = 1.766029949、B = 159531.024 nm²和C = -1.078×10¹⁰ nm⁴时,结果与理论数据令人满意地相关。已对该玻璃进行了X射线衍射(XRD)、傅里叶变换红外光谱(FT - IR)、差示扫描量热仪(DSC)曲线的测量。FT - IR曲线表明该玻璃同时具有BO₃和BO₄单元。从DSC热谱图中确定了玻璃转变温度(T(g))、结晶温度(T(c))和熔化温度(T(m)),并据此计算出了玻璃的其他相关参数。45B₂O₃ - 5ZnO - (50 - x)PbO - xCuO(x = 0、1、0.2、0.5和1.0 mol%)的可见吸收光谱分别在400 nm((²B₁g)-->(²E(g)))和780 nm((²B₁g)-->(²B₂g))处显示出Cu²⁺离子的两个吸收带。对于掺杂1 mol% CuO的玻璃,在306和332 nm激发下,发现了422和512 nm处的发射带。