Suppr超能文献

两种自酸蚀底漆/粘合剂系统的剪切粘结强度比较。

Comparison of shear bond strength of two self-etch primer/adhesive systems.

作者信息

Bishara Samir E, Ajlouni Raed, Laffoon John F, Warren John J

机构信息

Orthodontic Department, College of Dentistry, University of Iowa, Iowa City, Iowa 52242, USA.

出版信息

Angle Orthod. 2006 Jan;76(1):123-6. doi: 10.1043/0003-3219(2006)076[0123:COSBSO]2.0.CO;2.

Abstract

Orthodontic brackets adhesive systems use three different agents, an enamel conditioner, a primer solution, and an adhesive resin. A unique characteristic of some new bonding systems is that they combine the conditioning, priming, and adhesive agents into a single application. The purpose of this study was to assess and compare the effects of using one-step and two-step self-etch primer/adhesive systems on the shear bond strength of orthodontic brackets. The brackets were bonded to extracted human molars according to one of two protocols. Group I (control): a two-step self-etch acidic primer/adhesive system was used, Transbond Plus was applied to the enamel surface as suggested by the manufacturer. The brackets were bonded with Transbond XT and light cured for 20 seconds. Group II: a one-step self-etch, self-adhesive resin cement system, Maxcem, was applied directly to the bracket. The self-etch primer/adhesive is made of two components that mix automatically during application. The brackets were then light cured for 20 seconds. The mean shear bond strength of the two-step acid-etch primer/adhesive was 5.9 +/- 2.7 Mpa and the mean for the one-step system was 3.1 +/- 1.7 MPa. The in vitro findings of this study indicated that the shear bond strengths (t = 3.79) of the two adhesive systems were significantly different (P = .001). One-step adhesive systems could potentially be advantageous for orthodontic purposes if their bond strength can be improved.

摘要

正畸托槽粘结系统使用三种不同的试剂,一种釉质调节剂、一种底漆溶液和一种粘结树脂。一些新型粘结系统的独特之处在于它们将调节、底漆和粘结剂组合在一次应用中。本研究的目的是评估和比较使用一步法和两步法自酸蚀底漆/粘结系统对正畸托槽剪切粘结强度的影响。根据两种方案之一将托槽粘结到拔除的人类磨牙上。第一组(对照组):使用两步法自酸蚀酸性底漆/粘结系统,按照制造商的建议将Transbond Plus应用于釉质表面。使用Transbond XT粘结托槽并光照固化20秒。第二组:将一步法自酸蚀、自粘结树脂水门汀系统Maxcem直接应用于托槽。自酸蚀底漆/粘结剂由两种成分组成,在应用过程中自动混合。然后将托槽光照固化20秒。两步法酸蚀底漆/粘结剂的平均剪切粘结强度为5.9±2.7MPa,一步法系统的平均剪切粘结强度为3.1±1.7MPa。本研究的体外研究结果表明,两种粘结系统的剪切粘结强度(t = 3.79)存在显著差异(P = .001)。如果一步法粘结系统的粘结强度能够提高,那么它可能对正畸目的具有优势。