Hirabayashi Katsuhiko, Kanbara Hirohisa, Mori Yuhei, Kurihara Takashi, Shimizu Masaki, Hiyama Tamejiro
NTT Photonics Laboratories, NTT Corporation, 3-1 Morinosato, Wakamiya, Atsugi-shi, Kanagawa 243-0198, Japan.
Appl Opt. 2007 Dec 10;46(35):8402-10. doi: 10.1364/ao.46.008402.
We developed a sensitive two-color-absorption photopolymer in which holograms are recorded by simultaneous irradiation with a 660 nm interference light and a 410 nm gate light. Doped with bis(silyl)pentathiophene as a two-color-photosensitive dye and 2,2-dimethoxy-2-phenylacetophenone as a radical photopolymerization initiator; its matrix contains low-refractive index binding polymers and high-refractive index monomers. The sensitivity and diffraction efficiency of 25 mum thick layers are from 1.2 x 10(-9) to 3.7 x 10(-9) cm2/mJ and from 1% to 4%. We made a three-photopolymer-layer waveguide structure, where each photopolymer layer and high-refractive index adhesive layer serves as a core layer and is sandwiched between two low-refractive index glass substrates that serve as clad layers. Gate light propagated through the adhesive layers, reference and object beams intersected the photopolymer layers, and different diffraction patterns could be written in each layer.
我们开发了一种灵敏的双色吸收光聚合物,其中全息图是通过用660nm干涉光和410nm门光同时照射来记录的。掺杂双(硅烷基)五噻吩作为双色光敏染料和2,2-二甲氧基-2-苯基苯乙酮作为自由基光聚合引发剂;其基质包含低折射率粘结聚合物和高折射率单体。25μm厚的层的灵敏度和衍射效率分别为1.2×10⁻⁹至3.7×10⁻⁹cm²/mJ和1%至4%。我们制作了一种三光聚合物层波导结构,其中每个光聚合物层和高折射率粘合层用作芯层,并夹在两个用作包层的低折射率玻璃基板之间。门光通过粘合层传播,参考光束和物光束与光聚合物层相交,并且可以在每层中写入不同的衍射图案。