Imre Arpád W, Schönhoff Monika, Cramer Cornelia
Institut für Physikalische Chemie, Universität Münster, Corrensstr. 28/30, D-48149 Münster, Germany.
J Chem Phys. 2008 Apr 7;128(13):134905. doi: 10.1063/1.2901048.
Ionically cross-linked polyelectrolyte complexes (PECs) of anionic poly(sodium 4-styrene sulfonate) (PSS) and cationic poly(diallyldimethylammonium chloride) (PDADMAC), xPSS.(1-x)PDADMAC, with molar fractions x ranging from 0.30 to 0.70, were prepared and subsequently dried. The PEC samples were analyzed by differential scanning calorimetry, and the ionic conductivity sigmadc of the samples was measured as a function of temperature by means of impedance spectroscopy. The thermograms display an endothermic peak in the temperature range of 90-143 degrees C, which is attributed to a glass transition of the PEC. The glass transition temperature Tg has a symmetric x dependence with a minimum at x=0.50. The temperature dependence of sigmadcT is not affected by the glass transition. The ionic conductivity of the samples before drying is three orders of magnitude larger than sigmadc after drying; nevertheless, their activation enthalpies are identical. Arrhenius parameters obtained from the systematic study of several PEC compositions are discussed. The ionic conductivity of the PSS-rich samples is significantly higher than sigmadc of PDADMAC-rich samples. This implies a relatively high Na+ mobility as compared to Cl(-) mobility in PEC. In contrast to the symmetric x dependence of Tg, the conductivity of PEC increases and the activation enthalpy decreases with increasing x in the investigated composition range. A strong x dependence of sigmadc is observed for PSS-rich PEC, which is attributed to a significant variation in the mobility of the charge carriers.
制备了阴离子型聚(4-苯乙烯磺酸钠)(PSS)和阳离子型聚(二烯丙基二甲基氯化铵)(PDADMAC)的离子交联聚电解质复合物(PEC),即xPSS·(1 - x)PDADMAC,其中摩尔分数x的范围为0.30至0.70,随后进行干燥。通过差示扫描量热法对PEC样品进行分析,并借助阻抗谱测量样品的离子电导率σdc随温度的变化。热重曲线在90 - 143℃温度范围内显示出一个吸热峰,这归因于PEC的玻璃化转变。玻璃化转变温度Tg对x呈对称依赖性,在x = 0.50时出现最小值。σdcT的温度依赖性不受玻璃化转变的影响。干燥前样品的离子电导率比干燥后的σdc大三个数量级;然而,它们的活化焓是相同的。讨论了从对几种PEC组成的系统研究中获得的阿伦尼乌斯参数。富含PSS的样品的离子电导率明显高于富含PDADMAC的样品的σdc。这意味着在PEC中,与Cl⁻迁移率相比,Na⁺迁移率相对较高。与Tg对x的对称依赖性相反,在所研究的组成范围内,PEC的电导率随着x的增加而增加,活化焓则降低。对于富含PSS的PEC,观察到σdc对x有强烈的依赖性,这归因于载流子迁移率的显著变化。