George Jinu Jacob, Sengupta Rajatendu, Bhowmick Anil K
Rubber Technology Centre, Indian Institute of Technology, Kharagpur 721302, India.
J Nanosci Nanotechnol. 2008 Apr;8(4):1913-21.
Commercially available multiwalled carbon nanotubes (MWNT) were chemically modified by amine, acid and silane and their ethylene vinyl acetate (EVA) based nanocomposites were prepared. Unmodified and modified nanotubes were characterized by thermogravimetry, X-ray diffraction, Raman spectroscopy, X-ray photoelectron spectroscopy and transmission electron microscopy. Early degradation of modified nanotubes from the thermogravimetry study proved the presence of functional groups on nanotube surface. Increase in D-band to G-band ratio and a shift in radial breathing mode peaks from the Raman spectra indicated the generation of surface defects due to functionalization and variation in van der Waals force of attraction between nanotube aggregates on modification. The unmodified nanotubes improved the tensile strength by 30% with 4 weight% of filler. Amine modification imparted further increase in strength due to the presence of functional groups on the nanotube surface and the subsequent better dispersion of the nanotubes in the polymer matrix. The silane treatment imparted maximum improvement in various properties of the nanocomposites. The nanotubes provided better thermal degradation stability and also higher thermal conductivity to virgin EVA. The results were well supported by the morphological as well as swelling study of the various samples.
对市售多壁碳纳米管(MWNT)进行胺、酸和硅烷化学改性,并制备了基于乙烯-醋酸乙烯酯(EVA)的纳米复合材料。通过热重分析、X射线衍射、拉曼光谱、X射线光电子能谱和透射电子显微镜对未改性和改性后的纳米管进行了表征。热重分析研究表明改性纳米管的早期降解证明了纳米管表面存在官能团。拉曼光谱中D带与G带比值的增加以及径向呼吸模式峰的位移表明,由于功能化以及改性后纳米管聚集体之间范德华吸引力的变化,产生了表面缺陷。未改性的纳米管在添加4重量%的填料时,拉伸强度提高了30%。由于纳米管表面存在官能团以及随后纳米管在聚合物基体中更好的分散,胺改性使强度进一步提高。硅烷处理使纳米复合材料的各种性能得到最大程度的改善。纳米管为原始EVA提供了更好的热降解稳定性以及更高的热导率。各种样品的形态学和溶胀研究结果很好地支持了这些结果。