Wang Lei, Jin Yi-Ying, Nie Yong-Feng, Liu Jian-Guo, Li Run-Dong
Department of Environmental Science and Engineering, Tsinghua University, Beijing 100084, China.
Huan Jing Ke Xue. 2009 Apr 15;30(4):1232-7.
An experimental work was carried out to investigate the effect of additives (clay and coal fly ash) and washing-pretreatment on the stabilization of critical heavy metals (Cd, Cu, Zn, Pb, Cr, Ni) during a sintering process of municipal solid waste incinerator (MSWI) fly ash. The proportions of the three constituents were varied to adjust the mixture compositions. The washing time were 8 h, 16 h and 24 h. The material was compacted in cylindrical specimens at 3 kN and treated at 1,100 degrees C for 4 h. When the clay content was increased to 70%, the stabilized ratio was increased from 16.96% to 28.42% for Cd, from 10.58% to 37.02% for Pb, from 46.38% to 55.14% for Cu, from 42.14% to 64.47% for Zn, but the stabilized ratio of Ni and Cr was decreased. When coal fly ash was increased in the MSWI fly ash, the stabilized ratio was decreased from 16.96% to 4.67% for Cd, increased from 46.86% to 81.43% for Cu, but the addition of coal fly ash did not increased the stabilized ratio of Zn, Pb, Ni and Cr. Washing pre-treatment increased the stabilized ratio of Cd, Cu and Pb significantly. The leaching behavior of the heavy metals in the sintered products was studied by the toxicity characteristic leaching procedure (TCLP), the results showed that the leaching concentration of the six heavy metals were very low.
开展了一项实验工作,以研究添加剂(黏土和粉煤灰)及水洗预处理对城市固体废弃物焚烧炉(MSWI)飞灰烧结过程中关键重金属(镉、铜、锌、铅、铬、镍)稳定性的影响。改变三种成分的比例来调整混合物组成。水洗时间分别为8小时、16小时和24小时。将材料在3千牛压力下压制成圆柱形试样,并在1100摄氏度下处理4小时。当黏土含量增加到70%时,镉的稳定率从16.96%提高到28.42%,铅从10.58%提高到37.02%,铜从46.38%提高到55.14%,锌从42.14%提高到64.47%,但镍和铬的稳定率下降。当MSWI飞灰中粉煤灰增加时,镉的稳定率从16.96%降至4.67%,铜从46.86%增至81.43%,但粉煤灰的添加并未提高锌、铅、镍和铬的稳定率。水洗预处理显著提高了镉、铜和铅的稳定率。采用毒性特性浸出程序(TCLP)研究了烧结产物中重金属的浸出行为,结果表明六种重金属的浸出浓度非常低。