Ikeda Masahiko, Kurokawa Hiroyasu, Sunada Noriatsu, Tamura Yukie, Takimoto Masayuki, Murayama Ryosuke, Ando Susumu, Miyazaki Masashi
Department of Operative Dentistry, Nihon University School of Dentistry, Chiyoda-ku, Tokyo, Japan.
J Oral Sci. 2009 Dec;51(4):527-34. doi: 10.2334/josnusd.51.527.
The purpose of this study was to investigate the effect of previous phosphoric acid etching on the dentin bond strength of single-step self-etch adhesive systems. Facial surfaces of bovine teeth were wet ground with #600 SiC paper. Adhesives were applied with and without previous phosphoric acid etching, and light irradiated. Resin composite was bonded to the adherend surface, followed by light irradiation and storage in water at 37 degrees C. Four groups (n = 10) were made per adhesive system: with and without previous acid etching and with and without thermal cycling between 5 degrees C and 55 degrees C for 10,000 cycles. Specimens were tested in a shear mode at a crosshead speed of 1.0 mm/min. Two-way ANOVA and Tukey HSD test at a level of 0.05 were performed. The changes in dentin bond strengths were different among the adhesive systems tested. In all experimental conditions of this study, the dentin bond strength decreased or remained unchanged with previous acid etching. From the results of this study, previous acid etching might not be acceptable for increasing dentin bond strength of the single-step self-etch adhesive systems.
本研究的目的是调查先前磷酸酸蚀对单步自酸蚀粘结系统牙本质粘结强度的影响。用#600碳化硅砂纸湿磨牛牙的颊面。在有和没有先前磷酸酸蚀的情况下施加粘结剂,并进行光照。将树脂复合体粘结到被粘结表面,随后进行光照并在37℃水中储存。每个粘结系统分为四组(n = 10):有和没有先前酸蚀,以及有和没有在5℃至55℃之间进行10000次循环的热循环。以1.0 mm/min的十字头速度在剪切模式下对试样进行测试。进行了水平为0.05的双向方差分析和Tukey HSD检验。在所测试的粘结系统中,牙本质粘结强度的变化各不相同。在本研究的所有实验条件下,先前酸蚀会使牙本质粘结强度降低或保持不变。从本研究结果来看,对于提高单步自酸蚀粘结系统的牙本质粘结强度而言,先前酸蚀可能是不可接受的。