Distortions in the marginal region during manufacture are detrimental to the long-term success of fixed dental prostheses (FDPs). The aim of the present in vitro study was to evaluate changes in marginal fit because of the veneering process of four-unit FDPs made from different zirconia materials. Two groups of FDPs with 10 specimens each were machined from white body zirconia blanks (VITA In-Ceram YZ Cubes, KaVo Everest ZS-Blanks) by means of computer-aided design/computer-aided manufacturing systems and subsequently sintered to their final density. The marginal and internal gaps of the frameworks were determined using a replica technique. Afterwards, frameworks were veneered with the recommended ceramics (VITA VM9, GC Initial Zr), and fitting accuracy was evaluated again. Statistical analyses were performed by Student's t-test with the level of significance chosen at 0.05. With one framework/veneering system (Everest ZS-Blanks/Initial Zr), both marginal gap (P = 0.019) and internal gap (P = 0.001) at the premolar retainer were significantly affected by the veneering process. The resulting distortions were directed towards the lumina of the retainers and the mean values of the measured gaps decreased by about 23.8 mum (marginal gap) and 27.3 mum (internal gap). For the other system (In-Ceram YZ Cubes/VM9), no distortions because of the veneering were found. The veneering of zirconia restorations may lead to significant changes in the marginal fit, while the combination of core and veneering material used influences the resulting distortions.

摘要

在制造过程中,边缘区域的变形会对固定义齿修复体(FDP)的长期成功产生不利影响。本体外研究的目的是评估由于不同氧化锆材料制成的四单位 FDP 的贴面过程而导致的边缘适合性的变化。从白色体氧化锆坯料(VITA In-Ceram YZ Cubes、KaVo Everest ZS-Blanks)通过计算机辅助设计/计算机辅助制造系统加工出两组各有 10 个试件的 FDP,然后将其烧结至最终密度。使用复制技术确定框架的边缘和内部间隙。之后,用推荐的陶瓷(VITA VM9、GC Initial Zr)对框架进行贴面,并再次评估贴合精度。使用 Student's t 检验进行统计分析,选择显著性水平为 0.05。对于一个框架/贴面系统(Everest ZS-Blanks/Initial Zr),贴面过程显著影响前磨牙保持器的边缘间隙(P = 0.019)和内部间隙(P = 0.001)。由此产生的变形指向保持器的腔,测量间隙的平均值减少了约 23.8 µm(边缘间隙)和 27.3 µm(内部间隙)。对于另一个系统(In-Ceram YZ Cubes/VM9),由于贴面没有发现变形。氧化锆修复体的贴面可能会导致边缘适合性的显著变化,而使用的核材料和贴面材料的组合会影响产生的变形。

文献AI研究员

20分钟写一篇综述,助力文献阅读效率提升50倍。

立即体验

用中文搜PubMed

大模型驱动的PubMed中文搜索引擎

马上搜索

文档翻译

学术文献翻译模型,支持多种主流文档格式。

立即体验