de Castro M C, Steagall L
Faculdade de Odontología da Universidade de São Paulo.
Rev Odontol Univ Sao Paulo. 1990 Oct-Dec;4(4):293-8.
This research evaluates the corrosion as expressed by the mass loss of experimental samples of both (conventional amalgam alloys (New True, Dentalloy and Velvalloy) and copper-rich alloys (Dispersalloy, Rezzizt II, Novaloy and Novaloy Plus) after immersion in a 1% NaCl solution. The sequence of treatments was: a) carved and burnished and b) carved, burnished and polished under uniform and controlled conditions the samples were weighed and alternatively submitted to immersion and finally brushed and weighed again after period of 30, 60 and 90 days. The polished samples exhibited a mass loss significantly lower than the burnished ones. The mass loss was statistically significant for the three experimental periods of time and presented a continuous mode. Differences among the alloys were detected either as to composition or surface treatment adapted.
本研究评估了(传统汞合金(New True、Dentalloy和Velvalloy)以及富铜合金(Dispersalloy、Rezzizt II、Novaloy和Novaloy Plus))实验样品在浸入1%氯化钠溶液后以质量损失表示的腐蚀情况。处理顺序为:a)雕刻和打磨,b)在均匀且可控的条件下进行雕刻、打磨和抛光。对样品进行称重,然后交替进行浸泡,在30天、60天和90天后最后再次进行刷洗并称重。经过抛光的样品质量损失明显低于经过打磨的样品。在三个实验时间段内质量损失具有统计学意义,且呈现出连续模式。在合金之间,无论是成分还是采用的表面处理方面均检测到了差异。