Suppr超能文献

激光脉冲形状和持续时间对损伤部位起始尺寸的影响以及对后续修复的影响。

The effect of laser pulse shape and duration on the size at which damage sites initiate and the implications to subsequent repair.

作者信息

Carr C W, Cross D A, Norton M A, Negres R A

机构信息

Lawrence Livermore National Laboratory, Livermore, California 94551, USA.

出版信息

Opt Express. 2011 Jul 4;19 Suppl 4:A859-64. doi: 10.1364/OE.19.00A859.

Abstract

Growth of laser damage on SiO(2) optical components used in high power lasers can be reduced or eliminated by pre-exposure to pulses of a few hundred ps in duration. Such pre-exposure would cause weak locations on the optics surface to self-identify by initiating very small damage sites. The sites which initiate will be only a few microns in diameter and will have a very low probability of growing even without any further treatment. Repairing damage sites when small is important because both laser mitigation and acid etching are very successful in preventing such small sites from growing.

摘要

通过预先暴露于持续时间为几百皮秒的脉冲,可以减少或消除高功率激光器中使用的SiO₂光学元件上激光损伤的增长。这种预先暴露会通过引发非常小的损伤部位,使光学表面的薄弱位置自我识别。引发的部位直径只有几微米,即使不进行任何进一步处理,其生长的可能性也非常低。在损伤部位还小时进行修复很重要,因为激光缓解和酸蚀刻在防止此类小部位生长方面都非常成功。