Suppr超能文献

通过表面印迹技术与溶胶-凝胶法相结合制备新型 Cu(II) 磁性离子印迹材料。

Novel Cu (II) magnetic ion imprinted materials prepared by surface imprinted technique combined with a sol-gel process.

机构信息

Key Laboratory of Jiangxi Province for Ecological Diagnosis-Remediation and Pollution Control, Nanchang 330063, PR China.

出版信息

J Hazard Mater. 2011 Sep 15;192(3):949-55. doi: 10.1016/j.jhazmat.2011.05.042. Epub 2011 Jul 7.

Abstract

A novel Cu (II) magnetic ion-imprinted polymer (MIIP) was synthesized by surface imprinting technique combined with a sol-gel process. The adsorbent of Cu (II)-MIIP shows higher capacity and selectivity than that of magnetic non-imprinted polymers (MNIP). Adsorption capacities of Cu (II)-MIIP and MNIP are 24.2 and 5.2mg/g for Cu (II) ions, respectively. The selectivity coefficients of the Cu (II)-MIIP for Cu (II)/Zn (II) and Cu (II)/Ni (II) are 91.84 and 133.92, respectively. Kinetics studies show that the adsorption process obeys pseudo-second-order rate mechanism with an initial adsorption rate of 132.48 for Cu (II)-MIIP and 2.41mgg(-1)min(-1) for MNIP. In addition, no obvious decrease was observed after up to five adsorption cycles, indicating that the Cu (II)-MIIP is of high stability.

摘要

一种新型的 Cu(II) 磁性离子印迹聚合物(MIIP)是通过表面印迹技术与溶胶-凝胶法相结合合成的。Cu(II)-MIIP 的吸附剂比磁性非印迹聚合物(MNIP)具有更高的容量和选择性。Cu(II)-MIIP 和 MNIP 对 Cu(II)离子的吸附容量分别为 24.2 和 5.2mg/g。Cu(II)-MIIP 对 Cu(II)/Zn(II)和 Cu(II)/Ni(II)的选择性系数分别为 91.84 和 133.92。动力学研究表明,吸附过程符合准二级速率机制,Cu(II)-MIIP 的初始吸附速率为 132.48,MNIP 的初始吸附速率为 2.41mgg(-1)min(-1)。此外,在多达五个吸附循环后,没有观察到明显的下降,表明 Cu(II)-MIIP 具有很高的稳定性。