State Key Laboratory of Silicon Materials and Department of Materials Science and Engineering, Zhejiang University, Hangzhou 310027, China.
Nanoscale. 2012 Sep 21;4(18):5724-30. doi: 10.1039/c2nr31397a. Epub 2012 Aug 13.
A porous NiO/RGO hybrid film is prepared by the combination of electrophoretic deposition and chemical-bath deposition. The porous hybrid film exhibits a noticeable electrochromism with reversible color changes from transparent to dark brown, and shows high coloration efficiency (76 cm(2) C(-1)), fast switching speed (7.2 s and 6.7 s) and better cycling performance compared with the porous NiO thin film. The enhancement of electrochromic performances are attributed to the reinforcement of the electrochemical activity of the RGO sheets and the greater amount of open space in the porous hybrid film which allows the electrolyte to penetrate and shorten the proton diffusion paths within the bulk of NiO.
采用电泳沉积和化学浴沉积相结合的方法制备了多孔 NiO/RGO 杂化薄膜。该多孔杂化薄膜表现出显著的电致变色性能,颜色可由透明变为深棕色,具有较高的着色效率(76cm(2)C(-1))、较快的响应速度(7.2s 和 6.7s)和较好的循环稳定性,优于多孔 NiO 薄膜。电致变色性能的提高归因于 RGO 片的电化学活性增强和多孔杂化薄膜中更多的开放空间,这使得电解质能够渗透并缩短 NiO 体相中的质子扩散路径。