Bioengineering Laboratory, RIKEN, Hirosawa 2-1, Wako, Saitama 351-0198, Japan.
Langmuir. 2012 Oct 9;28(40):14347-56. doi: 10.1021/la303128y. Epub 2012 Sep 26.
Linear and miktoarm star-shaped diblock copolymers consisting of single-stranded DNA and poly(N-isopropylacrylamide) (PNIPAAm) with various compositions were synthesized via atom transfer radical polymerization and click chemistry. The temperature-responsive phase transition behavior, micellization, was systematically examined using UV-vis spectrometry, high-sensitivity differential scanning calorimetry, dynamic light scattering, and small-angle X-ray scattering. The lower critical solution temperature (LCST) increased, and its enthalpy decreased with decreasing PNIPAAm content. The copolymers self-assembled into well-defined nanoparticles having a core composed of PNIPAAm and a coronal layer of DNA above LCST. The particle size and micellar aggregation number of copolymer chains depended on the macromolecular composition and chain architecture. On the other hand, regardless of their factors, the surface area occupied by one DNA strand was found to be almost unchanged. The hybridization of DNA on the nanoparticles with fully complementary one induced the aggregation of the particles in a non-cross-linking configuration. The nanoparticle composed of miktoarm star copolymer showed a quicker DNA-hybridization response in this non-cross-linking aggregation compared with the case of a linear analogue.
通过原子转移自由基聚合和点击化学,合成了由单链 DNA 和聚(N-异丙基丙烯酰胺)(PNIPAAm)组成的线性和多臂星形嵌段共聚物,具有不同的组成。使用紫外可见光谱法、高灵敏度差示扫描量热法、动态光散射和小角 X 射线散射系统地研究了温度响应相转变行为、胶束化。随着 PNIPAAm 含量的降低,LCST 升高,其焓值降低。共聚物自组装成具有 PNIPAAm 核和 LCST 以上 DNA 冠状层的明确定义的纳米粒子。共聚物链的粒径和胶束聚集数取决于大分子组成和链结构。另一方面,无论其因素如何,发现一条 DNA 链占据的表面积几乎保持不变。与线性类似物相比,在非交联构象中,完全互补的纳米粒子上的 DNA 杂交诱导了粒子的聚集。与线性类似物相比,在这种非交联聚集中,由多臂星形共聚物组成的纳米粒子显示出更快的 DNA 杂交响应。