da Rosa Ricardo Abreu, Barreto Mirela Sangoi, da Rosa Tiago Abreu, Reis Katia Rodrigues, Kaizer Osvaldo Bazzan
School of Dentistry, Rio Grande do Sul Federal University, Porto Alegre, Brazil.
Gen Dent. 2013 Mar-Apr;61(2):45-9.
This study used differential root weakening to evaluate the fracture resistance of bovine teeth restored using glass fiber posts (with or without accessory glass fiber posts). Fifty bovine mandibular incisors were sectioned 14 mm from the apex, fixed in acrylic resin blocks, and divided into 5 groups: healthy roots with a glass fiber post (Group 1), partially weakened teeth with a glass fiber post (Group 2), partially weakened teeth with a glass fiber post and 2 accessory glass fiber posts (Group 3), extensively weakened teeth with a glass fiber post (Group 4), and extensively weakened teeth with a glass fiber post and 5 accessory glass fiber posts (Group 5). Posts were luted with resin cement, cores were prepared using composite resin, and metallic crowns were cemented. The specimens were stored in distilled water at 37°C for more than 72 hours until the fracture resistance test. Specimens were loaded at 135 degrees relative to the long axis of the tooth at a crosshead speed of 0.5 mm/minute in a universal testing machine. All groups predominantly exhibited favorable failure patterns and there were no statistically significant differences between groups (two-way ANOVA, α = 0.05).
本研究采用差异牙根弱化法评估使用玻璃纤维桩(有无辅助玻璃纤维桩)修复的牛牙的抗折性能。将50颗牛下颌切牙从根尖处截下14毫米,固定于丙烯酸树脂块中,并分为5组:有玻璃纤维桩的健康牙根(第1组)、有玻璃纤维桩的部分弱化牙(第2组)、有玻璃纤维桩和2根辅助玻璃纤维桩的部分弱化牙(第3组)、有玻璃纤维桩的广泛弱化牙(第4组)、有玻璃纤维桩和5根辅助玻璃纤维桩的广泛弱化牙(第5组)。用树脂水门汀粘结桩,用复合树脂制备核,并粘结金属冠。将标本在37℃的蒸馏水中保存72小时以上,直至进行抗折性能测试。在万能试验机中,以相对于牙长轴135度的角度、0.5毫米/分钟的十字头速度对标本加载。所有组主要表现出良好的失效模式,组间无统计学显著差异(双向方差分析,α = 0.05)。