Saatchi Masoud, Shadmehr Elham, Talebi Seyed Morteza, Nazeri Mohsen
Torabinejad Dental Research Center, Department of Endodontics, Dental School, Isfahan University of Medical Sciences, Isfahan, Iran.
Iran Endod J. 2013 Summer;8(3):85-8. Epub 2013 Aug 1.
The purpose of this clinical study was to compare the blood mercury levels before and after endodontic surgery using amalgam as a root-end filling material.
Fourteen patients requiring periradicular surgery participated in this prospective clinical study. A zinc-free amalgam was employed as root-end filling material. Blood samples were collected at three intervals: immediately before, immediately after and one week postoperatively. Mercury content of the blood was determined using gold amalgamation cold-vapor atomic absorption spectrometry. Obtained data were analyzed using analysis of variance for repeated measures and paired t-test.
The mean (SD) of blood mercury levels was 2.20 (0.24) ng/mL immediately before surgery, 2.24 (0.28) ng/mL immediately after surgery and 2.44 (0.17) ng/mL one week after the periradicular surgery. The blood mercury level one week post-operative was significantly higher than both blood mercury levels immediately before (P<0.001) and immediately after (P=0.005) the surgery.
Placement of an amalgam retroseal during endodontic surgery can increase blood mercury levels after one week. The mercury levels however, are still lower than the toxic mercury levels. We suggest using more suitable and biocompatible root-end filling materials.
本临床研究的目的是比较使用汞合金作为根尖倒充填材料进行牙髓外科手术后患者的血液汞含量。
14例需要进行根尖周手术的患者参与了这项前瞻性临床研究。采用无锌汞合金作为根尖倒充填材料。在三个时间点采集血样:手术前即刻、手术后即刻和术后一周。采用金汞齐化冷蒸气原子吸收光谱法测定血液中的汞含量。使用重复测量方差分析和配对t检验对获得的数据进行分析。
手术前即刻血液汞含量的均值(标准差)为2.20(0.24)ng/mL,手术后即刻为2.24(0.28)ng/mL,根尖周手术后一周为2.44(0.17)ng/mL。术后一周的血液汞含量显著高于手术前即刻(P<0.001)和手术后即刻(P=0.005)的血液汞含量。
牙髓外科手术中使用汞合金进行根尖倒充填会使术后一周的血液汞含量升高。然而,汞含量仍低于有毒汞含量水平。我们建议使用更合适且生物相容性更好的根尖倒充填材料。