Department of Chemistry, University of California, Berkeley, California 94720, USA.
J Am Chem Soc. 2013 Aug 28;135(34):12560-3. doi: 10.1021/ja406497s. Epub 2013 Aug 16.
The surface structure of Pt(557) during the catalytic oxidation of hydrogen was studied with in situ scanning tunneling microscopy and X-ray photoelectron spectroscopy. At 298 K, the surface Pt oxide formed after exposing Pt(557) to approximately 1 Torr of O2 can be readily removed by H2, at H2 partial pressures below 50 mTorr. Water is detected as the product in the gas phase, which also coadsorbs with hydroxyl groups on the Pt(557) surface.