Yuan Fu-song, Sun Yu-chun, Xie Xiao-yan, Wang Yong, Lv Pei-jun
Center of Digital Dentistry, National Engineering Laboratory for Digital and Material Technology of Stomatology, Peking University School and Hospital of Stomatology Beijing 100081, China.
Department of Radiology, Peking University School and Hospital of Stomatology Beijing 100081, China.
Beijing Da Xue Xue Bao Yi Xue Ban. 2013 Dec 18;45(6):989-92.
To quantitatively evaluate the artifacts appearance of eight kinds of common dental restorative materials, such as zirconia.
For the full-crown tooth preparation of mandibular first molar, eight kinds of full-crowns, such as zirconia all-ceramic crown, glass ceramic crown, ceramage crown, Au-Pt based porcelain-fused-metal (PFM) crown, Pure Titanium PFM crown, Co-Cr PFM crown, Ni-Cr PFM crown, and Au-Pd metal crown were fabricated. And natural teeth in vitro were used as controls. These full-crown and natural teeth in vitro were mounted an ultraviolet-curable resin fixed plate. High resolution cone beam computed tomography (CBCT) was used to scan all of the crowns and natural teeth in vitro, and their DICOM data were imported into software MIMICS 10.0. Then, the number of stripes and the maximum diameters of artifacts around the full-crowns were evaluated quantitatively in two-dimensional tomography images.
In the two-dimensional tomography images,the artifacts did not appear around the natural teeth in vitro, glass ceramic crown, and ceramage crown. But thr artifacts appeared around the zirconia all-ceramic and metal crown. The number of stripes of artifacts was five to nine per one crown. The maximum diameters of the artifacts were 2.4 to 2.6 cm and 2.2 to 2.7 cm.
In the two-dimensional tomography images of CBCT, stripe-like and radical artifacts were caused around the zirconia all-ceramic crown and metal based porcelain-fused-metal crowns. These artifacts could lower the imaging quality of the full crown shape greatly. The artifact was not caused around the natural teeth in vitro, glass ceramic crown, and ceramage crown.
定量评估氧化锆等八种常见牙科修复材料的伪影表现。
对下颌第一磨牙进行全冠牙体预备,制作氧化锆全瓷冠、玻璃陶瓷冠、瓷睿刻全瓷冠、金铂合金烤瓷熔附金属冠(PFM)、纯钛PFM冠、钴铬PFM冠、镍铬PFM冠和金钯金属冠等八种全冠。以体外天然牙作为对照。将这些全冠和体外天然牙安装在紫外线固化树脂固定板上。使用高分辨率锥形束计算机断层扫描(CBCT)对所有全冠和体外天然牙进行扫描,并将其DICOM数据导入MIMICS 10.0软件。然后,在二维断层图像中定量评估全冠周围伪影的条纹数量和最大直径。
在二维断层图像中,体外天然牙、玻璃陶瓷冠和瓷睿刻全瓷冠周围未出现伪影。但氧化锆全瓷冠和金属冠周围出现了伪影。每个冠的伪影条纹数量为5至9条。伪影的最大直径为2.4至2.6厘米和2.2至2.7厘米。
在CBCT的二维断层图像中,氧化锆全瓷冠和金属基烤瓷熔附金属冠周围会产生条纹状和放射状伪影。这些伪影会大大降低全冠外形的成像质量。体外天然牙、玻璃陶瓷冠和瓷睿刻全瓷冠周围未产生伪影。