Chitosan-coated calcium silicate hydrate (CSH/chitosan) mesoporous microspheres formed by self-assembly of nanosheets have been synthesized in aqueous solution under ambient conditions without using any toxic surfactant or organic solvent. The method reported herein has advantages of simplicity, low cost and being environmentally friendly. The BET specific surface area of CSH/chitosan mesoporous microspheres is measured to be as high as ~356 m(2) g(-1), which is considerably high among calcium silicate materials. The as-prepared CSH/chitosan mesoporous microspheres are promising adsorbent and exhibit a quick and highly efficient adsorption behavior toward heavy metal ions of Ni(2+), Zn(2+), Cr(3+), Pb(2+) Cu(2+) and Cd(2+) in aqueous solution. The adsorption kinetics can be well fitted by the pseudo second-order model. The maximum adsorption amounts of Ni(2+), Zn(2+), Pb(2+), Cu(2+) and Cd(2+) on CSH/chitosan mesoporous microspheres are extremely high, which are 406.6, 400, 796, 425 and 578 mg/g, respectively. The CSH/chitosan adsorbent exhibits the highest affinity for Pb(2+) ions among five heavy metal ions. The adsorption capacities of the CSH/chitosan adsorbent toward heavy metal ions are relatively high compared with those reported in the literature.
壳聚糖包覆的硅酸钙水合物(CSH/壳聚糖)介孔微球是通过在水相中自组装纳米片在环境条件下合成的,无需使用任何有毒表面活性剂或有机溶剂。本报告所采用的方法具有简单、低成本和环保的优点。CSH/壳聚糖介孔微球的 BET 比表面积高达约 356 m²/g,在硅酸钙材料中相当高。所制备的 CSH/壳聚糖介孔微球是一种很有前途的吸附剂,对水溶液中的重金属离子 Ni(2+)、Zn(2+)、Cr(3+)、Pb(2+)、Cu(2+)和 Cd(2+)具有快速高效的吸附性能。吸附动力学可以很好地拟合伪二级模型。CSH/壳聚糖介孔微球对 Ni(2+)、Zn(2+)、Pb(2+)、Cu(2+)和 Cd(2+)的最大吸附量非常高,分别为 406.6、400、796、425 和 578 mg/g。CSH/壳聚糖吸附剂对 Pb(2+)离子的亲和力最高。与文献报道的相比,CSH/壳聚糖吸附剂对重金属离子的吸附容量相对较高。