Suppr超能文献

棕榈树纤维素的提取及其通过接枝共聚进行功能化

Extraction of palm tree cellulose and its functionalization via graft copolymerization.

作者信息

Al-Hoqbani Abdulmajeed A, Abdel-Halim E S, Al-Deyab Salem S

机构信息

Petrochemical Research Chair, Chemistry Department, College of Science, King Saud University, PO Box 2455, Riyadh 11451, Saudi Arabia.

Petrochemical Research Chair, Chemistry Department, College of Science, King Saud University, PO Box 2455, Riyadh 11451, Saudi Arabia.

出版信息

Int J Biol Macromol. 2014 Sep;70:275-83. doi: 10.1016/j.ijbiomac.2014.07.009. Epub 2014 Jul 11.

Abstract

The work in this paper was planned with the aim of extracting the cellulosic component of palm tree waste and functionalizing this cellulose through graft copolymerization with acrylic acid. The cellulose extraction included hot alkali treatment with aqueous sodium hydroxide to remove the non-cellulosic binding materials. The alkali treatment was followed by an oxidative bleaching using peracid/hydrogen peroxide mixture with the aim of removing the rest of non-cellulosic materials to improve the fiber hydrophilicity and accessibility towards further grafting reaction. Optimum conditions for cellulose extraction are boiling in 5% (W/V) NaOH in a material to liquor ratio of 1:20 for 1 h then bleaching with 60 ml/l bleaching mixture at initial pH value of 6.5 for 30 min. The pH of the bleaching medium is turned to the alkaline range 11 and bleaching continues for extra 30 min. Graft copolymerization reaction was initiated by potassium bromate/thiourea dioxide redox system. Optimum conditions for grafting are 30 mmol of potassium bromate, 30 mmol of thiourea dioxide and 150 g of acrylic acid (each per 100 g of cellulose). The polymerization reaction was carried out for 120 min at 50°C using a material to liquor ratio of 1:20.

摘要

本文的工作旨在提取棕榈树废料中的纤维素成分,并通过与丙烯酸的接枝共聚作用使这种纤维素功能化。纤维素提取包括用氢氧化钠水溶液进行热碱处理以去除非纤维素结合材料。碱处理之后是使用过酸/过氧化氢混合物进行氧化漂白,目的是去除其余的非纤维素材料,以提高纤维的亲水性和对进一步接枝反应的可及性。纤维素提取的最佳条件是在5%(W/V)的氢氧化钠中以1:20的料液比煮沸1小时,然后用60 ml/l的漂白混合物在初始pH值为6.5的条件下漂白30分钟。将漂白介质的pH值调至碱性范围11并继续漂白30分钟。接枝共聚反应由溴酸钾/二氧化硫脲氧化还原体系引发。接枝的最佳条件是30 mmol的溴酸钾、30 mmol的二氧化硫脲和150 g的丙烯酸(每100 g纤维素各为上述用量)。聚合反应在50°C下以1:20的料液比进行120分钟。

文献AI研究员

20分钟写一篇综述,助力文献阅读效率提升50倍。

立即体验

用中文搜PubMed

大模型驱动的PubMed中文搜索引擎

马上搜索

文档翻译

学术文献翻译模型,支持多种主流文档格式。

立即体验