Abstract

Activated carbon foam was successfully prepared from phenolic resin synthesized with phenol and formaldehyde under alkali condition. The influence of process variables, such as steam rate, carbonization temperature, carbonization time, activation temperature and activation time on the adsorption capacities of the activated carbon foam was studied. Under the optimum experimental conditions, the activated carbon foam with a specific surface area 727.62 m(2)/g was obtained. Moreover, the iodine value and carbon tetrachloride value of the activated carbon foam was 1050.28 mg/g and 401.37 mg/g, respectively. The pore size of the activated carbon foam was in the range of 3.5-5 nm which was determined through the N2 adsorption test. In addition, the yield of the activated carbon foam was 36.24%. The result of scanning electron microscopy (SEM) showed that the activated carbon foam became honeycomb structure, and its pore wall was thinner and smoother compared to the unactivated carbon foam.

摘要

以苯酚和甲醛在碱性条件下合成的酚醛树脂为原料,成功制备了活性炭泡沫。研究了蒸汽流量、碳化温度、碳化时间、活化温度和活化时间等工艺变量对活性炭泡沫吸附性能的影响。在最佳实验条件下,获得了比表面积为727.62 m²/g的活性炭泡沫。此外,活性炭泡沫的碘值和四氯化碳值分别为1050.28 mg/g和401.37 mg/g。通过N₂吸附试验确定,活性炭泡沫的孔径在3.5 - 5 nm范围内。另外,活性炭泡沫的产率为36.24%。扫描电子显微镜(SEM)结果表明,活性炭泡沫呈蜂窝状结构,与未活化的碳泡沫相比,其孔壁更薄且更光滑。