Koç Esra, Öngül Değer, Şermet Bülent
Department of Prosthodontics, Faculty of Dentistry, Istanbul Aydın University.
Dent Mater J. 2016;35(3):447-53. doi: 10.4012/dmj.2015-252.
This study evaluated fabrication techniques of recently introduced all-ceramic copings' marginal adaptation on two different implant abutments with different finish lines. Five different copings were prepared (Casted chrome-cobalt metal coping, Zirkonzahn, Cercon, In Ceram Alumina and IPS e.max Press) on two cementable implant abutments with two marginal designs. Ten samples for each coping group were prepared (totally 100 samples). Copings were cemented to implant abutments and marginal gap measurements were done from 24 points with stereomicroscope and the datas were analyzed by the Kruskal-Wallis test before cementation. Cercon copings showed the lowest marginal fit scores and metal copings showed the highest scores. After cementation, all marginal gap values have been increased. All marginal gap values obtained from crown copings can be considered in clinically acceptable limits (<120 µm) except metal copings after cementation on abutment with 135 degrees shoulder group (123 µm).
本研究评估了最近推出的全瓷冠边缘适配性的制作技术,该技术应用于两种具有不同边缘设计的不同种植体基台上。在两种具有两种边缘设计的可粘结种植体基台上制备了五种不同的冠(铸造铬钴金属冠、Zirkonzahn冠、Cercon冠、In Ceram氧化铝冠和IPS e.max Press冠)。为每个冠组制备了10个样本(共100个样本)。将冠粘结到种植体基台上,并使用体视显微镜从24个点进行边缘间隙测量,在粘结前通过Kruskal-Wallis检验对数据进行分析。Cercon冠显示出最低的边缘适配分数,金属冠显示出最高的分数。粘结后,所有边缘间隙值均增加。除了在135度肩台组基台上粘结后的金属冠(123 µm)外,从冠获得的所有边缘间隙值均可视为临床可接受范围(<120 µm)。