Li G Z, Liu F H, Chu Z S, Wu D M, Yang L B, Li J L, Wang M N, Wang Z L
J Nanosci Nanotechnol. 2016 Apr;16(4):3914-20. doi: 10.1166/jnn.2016.11862.
SiO2@Y2MoO6:Eu3+ core-shell phosphors were prepared by the sol-gel process. X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FT-IR), field emission scanning electron microscopy (FESEM), energy-dispersive X-ray spectra (EDS), transmission electron microscopy (TEM), photoluminescence (PL) spectra as well as kinetic decays were used to characterize the resulting SiO2@Y2MoO6:Eu3+ core-shell phosphors. The XRD results demonstrated that the Y2MoO6:Eu3+ layers on the SiO2 spheres crystallized after being annealed at 700 °C and the crystallinity increased with raising the annealing temperature. The obtained core-shell phosphors have spherical shape with narrow size distribution (average size ca. 640 nm), non-agglomeration, and smooth surface. The thickness of the Y2MoO6:Eu3+ shells on the SiO2 cores could be easily tailored by varying the number of deposition cycles (70 nm for four deposition cycles). The Eul+ shows a strong PL emission (dominated by 5D0-7F2 red emission at 614 nm) under the excitation of 347 nm UV light. The PL intensity of Eu3+ increases with increasing the annealing temperature and the number of coating cycles.
通过溶胶 - 凝胶法制备了SiO₂@Y₂MoO₆:Eu³⁺核壳结构荧光粉。利用X射线衍射(XRD)、傅里叶变换红外光谱(FT - IR)、场发射扫描电子显微镜(FESEM)、能量色散X射线光谱(EDS)、透射电子显微镜(TEM)、光致发光(PL)光谱以及动力学衰减来表征所得的SiO₂@Y₂MoO₆:Eu³⁺核壳结构荧光粉。XRD结果表明,SiO₂球上的Y₂MoO₆:Eu³⁺层在700℃退火后结晶,且结晶度随退火温度升高而增加。所获得的核壳结构荧光粉呈球形,尺寸分布窄(平均尺寸约640nm),无团聚且表面光滑。通过改变沉积循环次数可轻松调整SiO₂核上Y₂MoO₆:Eu³⁺壳层的厚度(四个沉积循环时为70nm)。在347nm紫外光激发下,Eu³⁺呈现出强烈的PL发射(以614nm处的⁵D₀→⁷F₂红色发射为主)。Eu³⁺的PL强度随退火温度和包覆循环次数的增加而增强。