College of Resources and Environment, Huazhong Agricultural University, Wuhan 430070, China; Department of Life Sciences and Technologies, Hubei Engineering University, Xiaogan 432000, China.
Department of Soil and Crop Sciences, Texas A&M University, College Station, TX 77843-2474, USA.
Int J Biol Macromol. 2016 Nov;92:1191-1196. doi: 10.1016/j.ijbiomac.2016.08.007. Epub 2016 Aug 4.
Chitosan-montmorillonite composites can provide hydrophobicity and amino groups to enhance the performances of montmorillonite in wastewater treatment. In this paper, low molar mass chitosan (LC) and medium molar mass chitosan (MC) were selected to intercalate a sodium montmorillonite (Mt). The adsorption isotherm of LC and MC on the Mt and the pH dependency were measured. Thermo X-ray diffraction (XRD) and Fourier transform infrared spectroscopy (FTIR) were used to characterize the chitosan-Mt composites. Results showed that with hydrochloric acid as the solvent of chitosans, increasing pH from 3 to 5.5 enhanced the adsorption of both LC and MC on the Mt, and when the equilibrium concentration of chitosans approached 300mg/L at pH 5.5, the amount of adsorbed chitosan reached the highest level of 0.203mg/mg for LC and 0.190mg/mg for MC, respectively. When the Mt was saturated with the chitosan, the amino groups on the chitosan were bonded with the Mt through electrostatic interaction and there was monolayer of the chitosan in the interlayer space of Mt, which were confirmed by FTIR spectra and XRD patterns, respectively.
壳聚糖-蒙脱石复合材料可以提供疏水性和氨基,以增强蒙脱石在废水处理中的性能。本文选择低相对分子质量壳聚糖(LC)和中相对分子质量壳聚糖(MC)来插层钠蒙脱石(Mt)。测量了 LC 和 MC 在 Mt 上的吸附等温线和 pH 值依赖性。热 X 射线衍射(XRD)和傅里叶变换红外光谱(FTIR)用于表征壳聚糖-Mt 复合材料。结果表明,以盐酸为壳聚糖的溶剂,pH 值从 3 增加到 5.5 会增强 LC 和 MC 在 Mt 上的吸附,当壳聚糖的平衡浓度在 pH 5.5 时接近 300mg/L 时,吸附的壳聚糖量达到最高水平,LC 为 0.203mg/mg,MC 为 0.190mg/mg。当 Mt 被壳聚糖饱和时,壳聚糖上的氨基通过静电相互作用与 Mt 键合,并且在 Mt 的层间空间中有一层壳聚糖,这分别通过 FTIR 光谱和 XRD 图谱得到证实。