Abstract

PURPOSE

To compare the survival, success rates, and biological/technical complications of posterior metal-ceramic (MC) and zirconia fixed partial dentures (FPDs).

MATERIALS AND METHODS

A total of 40 patients requiring 40 posterior FPDs were randomly assigned to receive 20 zirconia and 20 MC restorations. The restorations were examined 1 week (baseline) and 1, 3, and 5 years after the end of treatment. Technical and biological outcomes were compared. Data were statistically analyzed using the Wilcoxon signed-rank and Mann-Whitney U tests.

RESULTS

The survival rates of both groups were 100%, and the success rates were 80% (zirconia) and 100% (MC). No biological complications were observed. Minor chipping was found in 20% of the zirconia restorations. No differences in periodontal parameters were observed between groups.

CONCLUSIONS

Zirconia FPDs exhibited the same survival rate (100%) as MC FPDs after 5 years; however, the success rate was 80%, because an increased rate of chipping was observed in zirconia restorations.

摘要

目的

比较后牙金属陶瓷(MC)和氧化锆固定修复体(FPD)的存活率、成功率和生物学/技术并发症。

材料和方法

共 40 名需要 40 个后牙 FPD 的患者被随机分配接受 20 个氧化锆和 20 个 MC 修复体。修复体在治疗结束后 1 周(基线)、1 年、3 年和 5 年进行检查。比较技术和生物学结果。使用 Wilcoxon 符号秩和 Mann-Whitney U 检验对数据进行统计学分析。

结果

两组的存活率均为 100%,成功率分别为 80%(氧化锆)和 100%(MC)。未观察到生物学并发症。20%的氧化锆修复体出现轻微碎裂。两组间牙周参数无差异。

结论

氧化锆 FPD 在 5 年后与 MC FPD 具有相同的存活率(100%);然而,成功率为 80%,因为在氧化锆修复体中观察到更高的碎裂率。