Peng Sheng, Li Huan, Shi Shuyun
Key Laboratory of Hunan Forest Products and Chemical Industry Engineering, Jishou University, Zhangjiajie 427000, China.
National & Local United Engineering Laboratory of Integrative Utilization Technology of Eucommiaulmoides, Jishou University, Jishou 416000, China.
Se Pu. 2019 Mar 8;37(3):293-298. doi: 10.3724/SP.J.1123.2018.11026.
Hydrophilic, magnetic molecularly imprinted resins (MMIRs) were fabricated inside FeO@mSiO pores by the one-pot copolycondensation of chlorogenic acid (CGA), resorcinol, melamine, and formaldehyde. The final porous MMIRs with larger numbers of surface recognition sites were obtained by removing mSiO. The successful preparation of MMIRs was confirmed using transmission electron microscopy, Fourier transform infrared spectroscopy, vibrating sample magnetometry, thermo-gravimetric analysis, and water contact angle analysis. The analyses suggest that the MMIRs have excellent hydrophilicity and magnetic solid-phase extraction efficiency. The MMIRs had a good adsorption capacity (50.87 mg/g), fast rate of adsorption (equilibrium was attained at 70 min), and specific recognition for CGA. The MMIRs, in combination with high performance liquid chromatography, were directly used for the selective extraction and determination of CGA in Duzhong brick tea. The limit of detection and recovery were 0.7 mg/L and 93.1%-109.4%, respectively, with relative standard deviations of less than 9.6%. The proposed strategy was extremely promising for the facile, rapid, and selective determination of CGA in real aqueous samples.
通过绿原酸(CGA)、间苯二酚、三聚氰胺和甲醛的一锅法共缩聚反应,在FeO@mSiO孔隙内制备了亲水性磁性分子印迹树脂(MMIRs)。通过去除mSiO获得了具有大量表面识别位点的最终多孔MMIRs。使用透射电子显微镜、傅里叶变换红外光谱、振动样品磁强计、热重分析和水接触角分析证实了MMIRs的成功制备。分析表明,MMIRs具有优异的亲水性和磁性固相萃取效率。MMIRs具有良好的吸附容量(50.87 mg/g)、快速的吸附速率(70分钟达到平衡)以及对CGA的特异性识别。MMIRs与高效液相色谱相结合,直接用于杜仲砖茶中CGA的选择性萃取和测定。检测限和回收率分别为0.7 mg/L和93.1%-109.4%,相对标准偏差小于9.6%。所提出的策略对于在实际水样中简便、快速和选择性地测定CGA极具前景。