Suppr超能文献

用可发泡木薯淀粉粘结的低密度木质刨花板:初步研究

Low Density Wood-Based Particleboards Bonded with Foamable Sour Cassava Starch: Preliminary Studies.

作者信息

Monteiro Sandra, Martins Jorge, Magalhães Fernão D, Carvalho Luísa

机构信息

LEPABE-Faculdade de Engenharia, Universidade do Porto, rua Dr. Roberto Frias, 4200-465 Porto, Portugal.

DEMAD-Department of Wood Engineering, Polytechnic Institute of Viseu, Campus Politécnico de Repeses, 3504-510 Viseu, Portugal.

出版信息

Polymers (Basel). 2016 Oct 8;8(10):354. doi: 10.3390/polym8100354.

Abstract

This work investigates the feasibility of producing low density particleboards using an adhesive system based on sour cassava starch, taking advantage of its adhesive and self-expansion properties. Relevant properties of the produced particleboards were evaluated according to European Standards including: density, internal bond, moisture content and thickness swelling. Low density particleboards were produced with densities between 207 kg/m³ and 407 kg/m³. The best performance corresponded to particleboard with a density of 318 kg/m³, an internal bond strength of 0.67 N/mm², and a thickness swelling of 8.7%. These values meet the standard requirements of general purpose lightweight boards for use in dry conditions. Heat post-treatment (24 h at 80 °C) led to lower internal bond strength, due to retrogradation (recrystallization of amylose and amylopectin chains upon cooling) causing higher rigidity of the starch binder. However, it showed to have a significant effect on decreasing the thickness swelling.

摘要

本研究利用酸木薯淀粉的粘合和自膨胀特性,探讨了使用基于酸木薯淀粉的粘合剂体系生产低密度刨花板的可行性。根据欧洲标准对所生产刨花板的相关性能进行了评估,包括:密度、内结合强度、含水率和厚度膨胀率。生产出了密度在207 kg/m³至407 kg/m³之间的低密度刨花板。性能最佳的刨花板密度为318 kg/m³,内结合强度为0.67 N/mm²,厚度膨胀率为8.7%。这些值符合干燥条件下通用轻质板的标准要求。热后处理(80℃下24小时)导致内结合强度降低,这是由于回生(冷却时直链淀粉和支链淀粉链的再结晶)使淀粉粘合剂的刚性更高。然而,它对降低厚度膨胀率有显著效果。

https://cdn.ncbi.nlm.nih.gov/pmc/blobs/960d/6432213/7219432b6499/polymers-08-00354-g001.jpg

文献AI研究员

20分钟写一篇综述,助力文献阅读效率提升50倍。

立即体验

用中文搜PubMed

大模型驱动的PubMed中文搜索引擎

马上搜索

文档翻译

学术文献翻译模型,支持多种主流文档格式。

立即体验