Department of Cariology and Operative Dentistry, Graduate School of Medical and Dental Sciences, Tokyo Medical and Dental University.
Department of Regenerative Dental Medicine, Tokushima University Graduate School of Biomedical Sciences.
Dent Mater J. 2021 Dec 1;40(6):1394-1402. doi: 10.4012/dmj.2021-101. Epub 2021 Jul 22.
The effect of long-term water storage on the regional ultimate tensile strength (UTS), water sorption (W) and water solubility (W) of conventional and bulk-fill resin composites at various depths was investigated. Composite specimens light-cured from one side were sectioned into beams corresponding to different depths (1-5 mm) and stored in water for 24 h, 1 week, 1 month, 6 months or 1 year. UTS increased during the first week and then gradually decreased over time, especially in deeper regions. Bulk-fill composites initially exhibited similar UTS at all depths, whereas the UTS of conventional composites at 1 mm and 5 mm differed significantly at all time points. W and W increased with depth and storage time, markedly at 3-5 mm after 1 month for conventional composites and after 6 months for bulk-fill composites. The signs of degradation at depths beyond 3 mm suggested that even bulk-fill composites have suboptimal properties in layers more than 3 mm in thickness.
研究了长期水储存对常规和块状填充树脂复合材料的区域极限拉伸强度(UTS)、吸水(W)和水溶性(W)的影响,这些复合材料在不同深度处从一侧进行光固化。将对应于不同深度(1-5mm)的试件切成梁,并在水中储存 24 小时、1 周、1 个月、6 个月或 1 年。UTS 在第一周内增加,然后随着时间的推移逐渐降低,特别是在更深的区域。块状填充复合材料在所有深度初始时表现出相似的 UTS,而常规复合材料在 1mm 和 5mm 处的 UTS 在所有时间点都有显著差异。W 和 W 随深度和储存时间的增加而增加,在 1 个月后常规复合材料在 3-5mm 处和 6 个月后块状填充复合材料在 3-5mm 处增加明显。在超过 3mm 的深度出现降解迹象表明,即使是块状填充复合材料在厚度超过 3mm 的层中也具有不理想的性能。