In the current investigation, the influence of the tool geometry, the position of the materials in the joint, the welding speed on the temperature and torque developed, and on the quality of the welds in dissimilar and tri-dissimilar T joints were analysed. The aluminium alloys used were AA2017-T4, AA6082-T6, and AA5083-H111 and the friction stir welds were performed with identical shoulder tools, but with either a pin with simple geometry or a pin with progressive geometry. Progressive pin tools proved to be a viable alternative in the production of dissimilar and tri-dissimilar welds, as they provide a larger tool/material friction area and a larger volume of dragged material, which promotes an increase in the heat generated and a good mixing of the materials in the stir zone, although they require a higher torque. Placing a stronger material on the advancing side also results in a higher temperature in the stir zone but requires higher torque too. The combination of these factors showed that tools with a progressive pin provide sound dissimilar and tri-dissimilar welds, unlike single-pin tools. The increase in the welding speed causes the formation of defects in the stir zone, even in tri-dissimilar welds carried out with a tool with a progressive pin, which impairs the fatigue strength of the welds.
在当前的研究中,分析了刀具几何形状、材料在接头中的位置、焊接速度对产生的温度和扭矩以及对不同材料和三元不同材料T形接头焊接质量的影响。所使用的铝合金为AA2017-T4、AA6082-T6和AA5083-H111,搅拌摩擦焊采用相同的肩部刀具,但销钉要么是简单几何形状,要么是渐进几何形状。渐进式销钉刀具被证明是生产不同材料和三元不同材料焊缝的可行替代方案,因为它们提供了更大的刀具/材料摩擦面积和更大体积的拖动材料,这促进了热量的增加以及搅拌区内材料的良好混合,尽管它们需要更高的扭矩。将强度更高的材料放置在前进侧也会导致搅拌区内温度更高,但同样也需要更高的扭矩。这些因素的综合表明,与单销刀具不同,具有渐进式销钉的刀具能提供良好的不同材料和三元不同材料焊缝。焊接速度的提高会导致搅拌区内出现缺陷,即使是使用具有渐进式销钉的刀具进行的三元不同材料焊缝也会如此,这会削弱焊缝的疲劳强度。